Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

M. Holland Company PC402R Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer M. Holland Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M. Holland Company PC402R Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High clarityHigh heat resistanceHigh impact resistanceGood mold releaseApplications: AppliancesContainersTable products
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
23/23°C; ASTM D792
Melt Flow 10 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Yield 58.6 MPa
8500 psi
ASTM D638
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Izod Impact, Notched 8.54 J/cm
16.0 ft-lb/in
73°F; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 128 °C
262 °F
Unannealed; ASTM D648
Descriptive Properties Value Comments
Characteristics Mold release
Forms Pellets
Processing Methods Injection molding
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved