Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SSAB Tunnplat Docol® 800 DL High-strength Steel

Category Metal , Ferrous Metal , Alloy Steel , Low Alloy Steel
Manufacturer SSAB Tunnplat AB
Trade Name Docol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SSAB Tunnplat Docol® 800 DL High-strength Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
In course of development.Data provided by SSAB Tunnplat.
Physical Properties Metric English Comments
Density 7.87 g/cc
0.284 lb/in³
Estimated by MatWeb
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 800 - 950 MPa
116000 - 138000 psi
Tensile Strength, Yield >= 550 MPa
>= 79800 psi
After bake hardening
390 - 540 MPa

@Strain 0.200 %
56600 - 78300 psi

@Strain 0.200 %
Elongation at Break >= 13 %
>= 13 %
A<sub>80</sub>
Bend Radius, Minimum >= 1.0 t
>= 1.0 t
90° bend
Component Elements Properties Metric English Comments
Aluminum, Al 0.040 %
0.040 %
Carbon, C 0.14 %
0.14 %
Iron, Fe 98 %
98 %
As remainder
Manganese, Mn 1.7 %
1.7 %
Niobium, Nb (Columbium, Cb) 0.015 %
0.015 %
Phosphorous, P 0.015 %
0.015 %
Silicon, Si 0.20 %
0.20 %
Sulfur, S 0.0020 %
0.0020 %
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved