Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 54.5 MPa | 7900 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding M4300 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 54.5 MPa | 7900 psi | ASTM D638 |
Polymer Resources PC/TP-GP1-[color]-3 PC Polyester, High Impact, Good Chemical Resistance, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 54.5 MPa | 7900 psi | ASTM D638 |
Polymer Resources PC-IM1 Polycarbonate, Impact Modified, Low Flow Polycarbonate, Impact Modified, Low FlowProcess: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided .. |
|||
Tensile Strength, Yield | 54.5 MPa | 7900 psi | ASTM D638 |
Polymer Resources PC-IM1-UV Polycarbonate, Impact Modified, Low Flow, UV-stabilized Polycarbonate, Impact Modified, Low Flow, UV-stabilizedProcess: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Tensile Strength, Yield | 54.5 MPa | 7900 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® XT EX3600-0002 UV Black Polycarbonate + PBT (PC+PBT) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Tensile Strength, Yield | 54.5 MPa | 7900 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® XT XT-100-BW01 Natural PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Tensile Strength, Yield | 54.5 MPa | 7900 psi | ASTM D638 |
Polymer Resources PC/TP-GP1 PC Polyester, High Impact, Good Chemical Resistance
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 54.5 MPa | 7900 psi | ASTM D638 |
Ravago Manufacturing Americas Hybrid B2026IU Polycarbonate + PBT Alloy Available in North America UV Stabilizer Good Impact Resistance RoHS Compliant Form: Pellets Processing Method: Injection Molding Information provided by Ravago |
|||
Tensile Strength, Yield | 54.5 MPa | 7900 psi | Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638 |
PolyOne Therma-Tech™ SF-5000C TC Polyphenylene Sulfide (PPS)
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Tensile Strength, Yield | 54.5 MPa | 7900 psi | ASTM D638 |
Global XNY-1424 Easy Flow Polycarbonate/Polyester Alloy Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 54.5 MPa | 7900 psi | ASTM D638 |
Techmer ES Luriblend® PC GF10 TS15 BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: PTFE + Silicone Lubricant(15%)Features: LubricatedAppearance: BlackInformation provided by T.. |
|||
Tensile Strength, Yield | 54.5 MPa | 7900 psi | ASTM Data |
Styron Pulse® B250 ABS + Polycarbonate PULSE® B250 Engineering resin has been designed to provide a customized balance of low coefficient of linear thermal expansion, low temperature toughness and Class A surface finish paintability. .. |
|||
Tensile Strength, Yield | 54.5 MPa | 7900 psi | ASTM D-638 |
Axiall ProTherm® 4353 Rigid PVC, Extrusion Georgia Gulf ProTherm® 4353 is a CPVC powder blend designed for extrusion of large diameter, heavy wall industrial pipe requiring high temperature and good chemical resistance. Processing and stab.. |
|||
Tensile Strength, Yield | 54.5 MPa | 7900 psi | ASTM D638 |
LNP Lubricomp® IBL-4416 Polyamide 6/12 Copolymer, Glass Bead Reinforced, Silicone Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Tensile Strength, Yield | 54.5 MPa | 7900 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding M4910 (USP CLASS VI for TRANS 9494 only) Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 54.5 MPa | 7900 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® XT XT-100-CX00 PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |