Material Notes:
Georgia Gulf 3121 is an exterior grade powder compound formulated for processing applications requiring high production output rate. Having excellent weatherability and impact strength, 3121 is suitable for such applications as windows, doors, decks and fencing.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 111
111
ASTM D-785
Hardness, Shore D 82
82
ASTM D-2240
Tensile Strength, Yield 45.0 MPa
6530 psi
ASTM D-638
Elongation at Yield 4.2 %
4.2 %
ASTM D-638
Tensile Modulus 2.72 GPa
395 ksi
ASTM D-638
Flexural Strength 76.46 MPa
11090 psi
ASTM D-790
Flexural Modulus 2.54 GPa
368 ksi
ASTM D-790
Izod Impact, Notched 2.30 J/cm

@Thickness 6.35 mm
4.30 ft-lb/in

@Thickness 0.250 in
ASTM D-256
11.2 J/cm

@Thickness 3.17 mm
21.0 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Tensile Impact Strength 210 kJ/m²
100 ft-lb/in²
ASTM D-1822
Thermal Properties Metric English Comments
CTE, linear 63.0 µm/m-°C

@Temperature 20.0 °C
35.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Deflection Temperature at 1.8 MPa (264 psi) 69.4 °C
157 °F
ASTM D-648
Descriptive Properties Value Comments
Cell Classification 13343
ASTM D-1784
14434323
ASTM D-4216
Users viewing this material also viewed the following: