Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 241 - 276 MPa @Strain 0.200 % |
35000 - 40000 psi @Strain 0.200 % |
|
Materion BrushCAST® 165C High Strength Casting Alloy (As Cast) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Yield | 241 - 276 MPa @Strain 0.200 % |
35000 - 40000 psi @Strain 0.200 % |
|
Materion BrushCAST® 165CT Fine Grain Casting Alloy (As Cast) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Yield | 241 - 310 MPa @Temperature 20.0 °C |
35000 - 45000 psi @Temperature 68.0 °F |
typical |
H.C. Starck Ultra 76 Alloy (Ta 2.5%W) Benefits: Significantly improved corrosion resistance in HCl and H2SO4 acids.Minimized hydrogen embrittlement rates compared to standard NRC®76Up to 100 times lower in HCl acidUp to 10 times low.. |
|||
Tensile Strength, Yield | 241 MPa | 35000 psi | |
Mueller Ecostreamâ„¢ GreenDropâ„¢ C27451 DZR Lead Free Plumbing Brass To further compliment its EcoStreamâ„¢ family of alloys, Mueller Brass Company has developed a dezincification resistant version of its GreenDropâ„¢ C27450 Lead Free Brass Alloy. This new allo.. |
|||
Tensile Strength, Yield | 241 MPa | 35000 psi | ASTM D638 |
Techmer ES HiFill® PA4/6 CF40 IM HS 40% Carbon Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites.. |
|||
Tensile Strength, Yield | 241 - 414 MPa @Strain 0.200 % |
35000 - 60000 psi @Strain 0.200 % |
|
Special Metals DURANICKEL® 301 (UNS N03301) Annealed Strip Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Annealed Strip specifically. Other property values are typical of annealed DURANICKEL® alloy 3.. |
|||
Tensile Strength, Yield | >= 241 MPa @Strain 0.200 % |
>= 35000 psi @Strain 0.200 % |
Min per ASTM B582; Sheet and Plate |
Special Metals INCONEL® G-3 Nickel Superalloy Data provided by the manufacturer, Special Metals. |
|||
Tensile Strength, Yield | 241 MPa | 35000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 LGF60 HS L BK 12 mm Availability: North AmericaForms: PelletsFiller/Reinforcement: Long Glass FiberAdditive: Lubricant and Heat StabilizerFeatures: Lubricated, Heat Stabilized and Good MoldabilityAppearance: BlackProce.. |
|||
Tensile Strength, Yield | 241 MPa | 35000 psi | ASTM D638 |
Techmer ES Plastiblend® PA6/6,6 GF60 HS L 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Copolymer and Lubricat.. |
|||
Tensile Strength, Yield | 241 MPa | 35000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF70 HS L BK 70% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 70% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N.. |
|||
Tensile Strength, Yield | 241 - 379 MPa @Strain 0.200 %, Thickness >=25.4 mm |
35000 - 55000 psi @Strain 0.200 %, Thickness >=1.00 in |
Turned Bars |
Schmolz + Bickenbach UGIMA® 303 Stainless Steel Bar Description: 303 UGIMA® is Ugitech’s improved machining grade produced only by Ugitech. It is identical in every way to regular 303, except with respect to machinability. 303 UGIMA® repre.. |
|||
Tensile Strength, Yield | >= 241 MPa | >= 35000 psi | |
Alcoa UltrAlloy® 6020-T651 Aluminum Weldability = B; Stress Corrosion Cracking Resistance = A; General Corrosion Resistance = B (A = best; E = worst). General 6020 characteristics and uses: Excellent machinability, high corrosion resi.. |
|||
Tensile Strength, Yield | 241 - 345 MPa | 35000 - 50000 psi | 0.2% offset |
Eagle Brass 240 Low Brass, 1/2 Hard CDA 240 has excellent ductility, corrosion resistance and strength which allows it to be deep drawn, etched, stamped, blanked and bent. Typical uses include musical instruments, battery caps, flexib.. |
|||
Tensile Strength, Yield | 241 - 483 MPa | 35000 - 70000 psi | 0.2% offset |
Eagle Brass 762 Nickel Silver 12%, 1/4 Hard 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Tensile Strength, Yield | 241 MPa @Strain 0.200 % |
35000 psi @Strain 0.200 % |
|
Crucible Steel 303 SE Chromium-Nickel Steel Crucible 303 SE is a non-hardenable austenitic chromium-nickel steel to which selenium has been added to improve machinability and non-galling characteristics. This grade is non-magnetic in the anne.. |
|||
Tensile Strength, Yield | 241 MPa @Strain 0.200 % |
35000 psi @Strain 0.200 % |
|
Crucible Steel 321 Chromium-Nickel Steel Crucible 321 is a non-hardenable, low carbon austenitic chromium-nickel steel which is particularly adaptable for parts fabricated by welding without postweld annealing for use at temperatures betwe.. |
|||
Tensile Strength, Yield | 241 - 359 MPa | 35000 - 52000 psi | |
Chicago Extruded Metals BioBrass® UNS C62300 Aluminum Bronze Finished product available as bar, rod, forged or shapes.Chicago Extruded Metal temper codes: H02, M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extr.. |
|||
Tensile Strength, Yield | 241 - 469 MPa | 35000 - 68000 psi | |
Chicago Extruded Metals BioBrass® UNS C64200 Aluminum Bronze Finished product available as bar, rod, forged, or shapes.Chicago Extruded Metal temper codes: H02, M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Ext.. |
|||
Tensile Strength, Yield | >= 241 MPa @Strain 0.200 % |
>= 35000 psi @Strain 0.200 % |
|
Carlson 317L 4N Austenitic Stainless Steel General DescriptionCarlson’s 317L, 317L 4, and 317L 4N are austenitic chromium-nickel-molybdenum stainless steels with alloy contents greater than the 316 grades. The additional chromium, nickel a.. |
|||
Tensile Strength, Yield | >= 241 MPa @Strain 0.200 % |
>= 35000 psi @Strain 0.200 % |
|
Carlson C 600 Nickel-Chromium-Iron Alloy Carlson Alloy C 600 is nickel-chromium alloy, developed for use in severely corrosive environments at elevated temperatures. The high nickel content of this alloy provides excellent resistance to c.. |
|||
Tensile Strength, Yield | >= 241 MPa @Strain 0.200 % |
>= 35000 psi @Strain 0.200 % |
|
Carlson C 600ESR Nickel-Chromium-Iron Alloy General DescriptionCarlson Alloy C 600 is nickel-chromium alloy, developed for use in severely corrosive environments at elevated temperatures. The high nickel content of this alloy provides excell.. |
|||
Tensile Strength, Yield | >= 241 MPa @Strain 0.200 % |
>= 35000 psi @Strain 0.200 % |
|
Carlson C 825 Nickel-Iron-Chromium Alloy General DescriptionCarlson Alloy C 825 is a nickel-iron-chromium alloy, developed for use in extremely corrosive environments. The nickel content of this alloy makes it resistant to chloride-ion st.. |
|||
Tensile Strength, Yield | 241 - 283 MPa @Strain 0.200 %, Thickness 1.02 - 1.78 mm |
35000 - 41000 psi @Strain 0.200 %, Thickness 0.0400 - 0.0700 in |
Annealed Condition |
AK Steel 409 Ferritic Stainless steel AK Steel 409 Stainless Steels are especially useful for applications where oxidation or corrosion protection beyond the capacity of carbon steel and some coated steels is needed. Current applicatio.. |
|||
Tensile Strength, Yield | 241 MPa @Strain 0.200 % |
35000 psi @Strain 0.200 % |
typical annealed |
ATI Allegheny Ludlum AL 409HP™ Ferritic Stainless Steel, UNS S40930 Type 409 ferritic stainless steel was introduced by Allegheny Ludlum in 1961 to provide improved oxidation and corrosion resistance for automotive exhaust systems in comparison to carbon automotive .. |
|||
Tensile Strength, Yield | >= 241 MPa @Strain 0.200 % |
>= 35000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Stainless Steel JS700® Alloy (UNS N08700) Allegheny Ludlum's Corrosion resistant engineering alloy, JS700®, is a high-alloy, fully austenitic, superaustenitic stainless steel. This alloy is a proven problem-solver in many applications whe.. |
|||
Tensile Strength, Yield | 241 MPa @Strain 0.200 % |
35000 psi @Strain 0.200 % |
|
ATI Allvac® Nickelvac® 400 UNS N04400 Nickel Superalloy Nickel-Copper solid solution alloy. Uses: Equipment for mineral acids, brines, alkalis, offshore engineering, marine applications.Property values are for samples in the metallurgical condition: 165.. |
|||
Tensile Strength, Yield | 241 MPa @Strain 0.200 % |
35000 psi @Strain 0.200 % |
|
ATI Allvac® Nickelvac® 690 UNS N06690 Nickel Superalloy Uses: Nuclear, mineral acids manufacturing and processing facilities, high-temperature gas-phase reactors.Property values are for samples in the metallurgical condition: 1825°F anneal.Information p.. |
|||
Tensile Strength, Yield | 241 MPa @Strain 0.200 %, Temperature 427 °C |
35000 psi @Strain 0.200 %, Temperature 801 °F |
|
Haynes Hastelloy® C-22® alloy, 6.4-19.1 mm thick plate, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |