Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 180 MPa | 26100 psi | ASTM D638 |
Nylene® PA6 Glass Filled 5243 HS Nylon 6 43% Glass Filled; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Tensile Strength, Yield | 180 MPa | 26100 psi | ISO 527-1/2 |
Radici Radilon® ARV300 (dry) Nylon 66 30% Glass-fiber reinforcedInformation provided by Radici group. |
|||
Tensile Strength, Yield | 180 MPa | 26100 psi | ISO 527, ASTM D638 |
Nilit Nilamid A3 H7 G7 35% Glass Reinforced PA66 Description: Nilamid A3 H7 G7 is a 35% glass fiber reinforced NYLON 66 with a high heat stabilization. This product combines good overall mechanical performance and impact strength with ease of proc.. |
|||
Tensile Strength, Yield | 180 MPa | 26100 psi | ISO 527, ASTM D638 |
Nilit Nilamid B3 H G6 30% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G6 is a general purpose, 30% glass fiber reinforced NYLON 6 with a combination of good mechanical performance, impact strength and processability. It is one of the most wid.. |
|||
Tensile Strength, Yield | 180 MPa | 26100 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM HU2400 PEI (Asia Pacific) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Tensile Strength, Yield | 180 MPa | 26100 psi | ASTM D638 |
SPS Guang Zhou PONYLâ„¢ 4001G30 GF30%-PA66 Characteristic: High mechanical properties, superior heat resistance, good dimensional stabilityApplications: Power tool, chassis and E/E partsInformation Provided by SPS (Guang Zhou) Ltd. |
|||
Tensile Strength, Yield | >= 180 MPa @Strain 0.200 % |
>= 26100 psi @Strain 0.200 % |
|
SSAB Tunnplat Docol® DC05 (Fe P05) Deep-drawing Steel Deep-drawing SteelComments: Docol - Cold Rolled Mild Steel. Property values are for cold-rolled steel; thicknesses 0.40 - 3.00 mm. Iron content is approximate - exact composition is not reported b.. |
|||
Tensile Strength, Yield | >= 180 MPa @Strain 0.200 % |
>= 26100 psi @Strain 0.200 % |
|
SSAB Tunnplat Docol® DC06 (Fe P06) Deep-drawing Steel Deep-drawing SteelComments: Docol - Cold Rolled Mild Steel. Property values are for cold-rolled steel; thicknesses 0.40 - 3.00 mm. Iron content is approximate - exact composition is not reported b.. |
|||
Tensile Strength, Yield | 180 MPa | 26100 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RF006XXY PA 66 LNP* Thermocomp* RF006XXY is a compound based on Nylon 66 containing 30% Glass Fiber. |
|||
Tensile Strength, Yield | 180 MPa | 26100 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem HU2400 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Tensile Strength, Yield | 180 MPa | 26100 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem HU2410 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications.
Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
Tensile Strength, Yield | 180 MPa | 26100 psi | dry; ISO 527 |
Ter Hell Plastic Terez® PA 6 7500 GF 30 Polyamide 6, 30% Glass Fiber Reinforced Description: Medium viscosity Polyamide 6, 30% glass fiber reinforced, good flowability, good impact resistance and bright natural color.Application: For molding parts with good stiffness and good.. |
|||
Tensile Strength, Yield | 180 MPa | 26100 psi | ASTM-D638 |
Polyram PlusTek PB300G33 Nylon 6, 33% Glass Fiber 33% glass fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 180 MPa | 26100 psi | ASTM-D638 |
Polyram PlusTek PB300G6 Nylon 6, 30% Glass Fiber 30% Glass-fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 180 MPa | 26100 psi | ASTM-D638 |
Polyram PlusTek PB306G6 Nylon 6, 30% Glass Fiber 30% glass-fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 180 MPa | 26100 psi | ASTM D638 |
Tipco Tipcofil® AG 800 - 40% Glass Fiber Reinforced Nylon-6 Compound, with High Heat Stability 40% Glass Reinforced Nylon-6 CompoundApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Tensile Strength, Yield | 180 MPa | 26100 psi | ISO 527-2 |
Tisan TISLAMID® 66 30% Glass Fiber Reinforced Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Tensile Strength, Yield | 180 MPa | 26100 psi | ASTM-D638 |
Polyram PlusTek PB310G6 Nylon 6, 33% Glass Fiber 33% glass fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 180 MPa | 26100 psi | ASTM D638, ISO R527 |
EPICHEM Epinyl PA 6 GF 30 H Polyamide 6, 30% Glass, Heat Stabilized Characteristics: medium viscosity, 30% glass fibre, heat stabilized |
|||
Tensile Strength, Yield | 180 MPa | 26100 psi | ASTM D638, ISO R527 |
EPICHEM Epinyl PA 6 GF 30 Polyamide 6, 30% Glass Characteristics: medium viscosity, 30% glass fibre, excellent mechanical properties |
|||
Tensile Strength, Yield | >= 180 MPa | >= 26100 psi | |
AK Steel Cold Rolled Carbon Steel, Dent Resistant (DR 180), SAE J2340 Type 180 A Information provided by AK Steel |
|||
Tensile Strength, Yield | 180 - 270 MPa | 26100 - 39200 psi | |
ArcelorMittal 15 High formability steel for drawing, Hot rolled Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used extensively in the automotive industry, both for visible and stru.. |
|||
Tensile Strength, Yield | 180 - 260 MPa | 26100 - 37700 psi | |
ArcelorMittal 16 High formability steel for drawing, Hot rolled Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used extensively in the automotive industry, both for visible and stru.. |
|||
Tensile Strength, Yield | 180 - 230 MPa | 26100 - 33400 psi | |
ArcelorMittal 180 BH Bake hardening steel, Cold rolled Available in the following: uncoated (HC180B), electroglavanized (HC180B+ZE) and Extragal®/Galvannealed (HC180BD+Z)Description: The composition and processing of these steels are designed to promot.. |
|||
Tensile Strength, Yield | 180 MPa | 26100 psi | Dry; ASTM D638 |
Asahi Kasei Leona® 13G25 25% Glass Filled Nylon 66 Enhanced strength, stiffness and durability; with 25% GF.Applications:Automotive parts Information provided by Asahi Kasei |
|||
Tensile Strength, Yield | 180 MPa | 26100 psi | Dry; ASTM D638 |
Asahi Kasei Leona® 14G25 25% Glass Filled Nylon 66 Enhanced strength and stiffness; with 25% GF. Superior heat aging resistance, fatigue resistance, and creep resistance.Applications:Mechanical and electrical parts, engine mounts and other under-the.. |
|||
Tensile Strength, Yield | 180 MPa | 26100 psi | 50 mm/min; ISO 527-1/-2 |
BASF Ultramid® A3WG10 BK 00564 50% Glass Filled PA66 (Conditioned) Description: 50% glass-fiber reinforced injection-molding grade with high heat aging resistance for technical articles of very high stiffness.Information provided by BASF |
|||
Tensile Strength, Yield | 180 MPa | 26100 psi | ISO 527-2 |
Solvay Specialty Polymers Ixef® 2060 Polyarylamide (PARA)
(discontinued **) Ixef 2060 is a 55% reinforced, general purpose polyarylamide compound. This compound exhibits improved vibration resistance, low warpage, and excellent surface finish. This grade has excellent prope.. |