Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 296 - 372 MPa | 42900 - 54000 psi | With 0% cold work |
OMG Americas GlidCop® AL-25 Dispersion Strengthened Copper GlidCop® AL-25 is copper that is dispersion strengthened with 0.5 wt% ultrafine particles of aluminum oxide. It is produced using an internal oxidation powder metallurgy process whereby aluminum o.. |
|||
Tensile Strength, Yield | 296 MPa @Diameter 12.7 mm |
42900 psi @Diameter 0.500 in |
|
Kaiser 6040 T6, T651 Rod & Bar 6040 is a lead-free alternative to 6262. The alloy offers very good machinability along with good corrosion resistance. It also has excellent coating acceptance (anodize response). It can be used in.. |
|||
Tensile Strength, Yield | 296 MPa @Strain 0.200 %, Temperature 316 °C |
42900 psi @Strain 0.200 %, Temperature 601 °F |
|
Haynes Ultimet® alloy, 1.6 mm sheet Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Tensile Strength, Yield | 296 MPa @Strain 0.200 %, Temperature 427 °C |
42900 psi @Strain 0.200 %, Temperature 801 °F |
|
Haynes Ultimet® alloy, 12.7-50.8 mm bar Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Tensile Strength, Yield | 296 - 407 MPa | 43000 - 59000 psi | 0.2% offset |
Eagle Brass 18665 MSP1, 1/4 Hard MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs.. |
|||
Tensile Strength, Yield | 296 - 372 MPa | 43000 - 54000 psi | 0.2% offset |
Eagle Brass 230 Red Brass, 1/2 Hard CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste.. |
|||
Tensile Strength, Yield | >= 296 MPa @Strain 0.200 % |
>= 43000 psi @Strain 0.200 % |
|
Carlson 926 Mo Austenitic Stainless Steel General DescriptionCarlson alloy 926 Mo is a “super-austenitic” 6% molybdenum stainless steel that provides excellent resistance to a variety of highly corrosive environments. This alloy performs.. |
|||
Tensile Strength, Yield | 296 - 331 MPa @Strain 0.200 % |
42900 - 48000 psi @Strain 0.200 % |
|
AK Steel 439 Ferritic Stainless steel AK Steel 439 has better oxidation and corrosion resistance than Type 409. This alloy also has optimum formability that is reproducible coil after coil and heat after heat. This provides special ad.. |