Material Notes:
Type 409 ferritic stainless steel was introduced by Allegheny Ludlum in 1961 to provide improved oxidation and corrosion resistance for automotive exhaust systems in comparison to carbon automotive exhaust systems in comparison to carbon steel. They alloy wad designated MF-1 indicating its end use: automotive mufflers. The good fabricability of this alloy, combined with its basic corrosion resistance and economy have significantly broadened the utility of Type 409.Since its introduction, the Type 409 alloy has been widely used in automotive exhaust systems for manifolds, exhaust pipes, catalytic converters, mufflers, tail pipes and other components. Type 409 stainless steel sheet has also found many other applications such as in culverts, home heating systems, automotive thermostats and fuel filters, electrical transformer cases, caskets, heat exchanger tubing, and various farm equipment components. Plate has been used as blades and vanes in standby power generation turbines and as jet engine sound-deadening devices at airports.The performance of Type 409 ferritic stainless steel in most applications has been excellent. However, some industry application have resulted in intergranular corrosion of weld heat-affected zones. The result of Allegheny Ludlum's research to investigate and redefine the balance of stabilizing elements is the AL 409HP stainless steel amounts of titanium and columbium which provide resistance to sensitization and intergranular corrosion which might occur in the heat affected zones of welds or in base metal following other thermal exposures. A low incidence of titanium nitride surface imperfections is also a characteristic of this alloy. The balance of stabilizing elements is designed to optimize weldability without need for post-weld annealing to restore ductility. Formability and toughness are also improved in comparison to the standard Type 409 alloy.This AL 409HP alloy is a proprietary stainless steel composition. Like all Type 409 alloys, the AL 409HP stainless steel contains nominally 11 percent chromium for greatly enhanced corrosion resistance in comparison to carbon steel. It is an excellent choice for all automotive exhaust system applications where 11 percent chromium provides sufficient resistance to oxidation and corrosion. Hot end exhaust applications may require an 18 percent chromium alloy.Information provided by Allegheny Ludlum
Physical Properties Metric English Comments
Density 7.76 g/cc
0.280 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 71
71
typical annealed
Tensile Strength, Ultimate 434 MPa
62900 psi
typical annealed
Tensile Strength, Yield 241 MPa

@Strain 0.200 %
35000 psi

@Strain 0.200 %
typical annealed
Elongation at Break 33 %

@Thickness 50.8 mm
33 %

@Thickness 2.00 in
typical anneal
Modulus of Elasticity 200 GPa
29000 ksi
Thermal Properties Metric English Comments
CTE, linear 10.52 µm/m-°C

@Temperature 20.0 - 100 °C
5.844 µin/in-°F

@Temperature 68.0 - 212 °F
11.11 µm/m-°C

@Temperature 20.0 - 260 °C
6.172 µin/in-°F

@Temperature 68.0 - 500 °F
11.88 µm/m-°C

@Temperature 20.0 - 482 °C
6.600 µin/in-°F

@Temperature 68.0 - 900 °F
Specific Heat Capacity 0.477 J/g-°C
0.114 BTU/lb-°F
Thermal Conductivity 25.0 W/m-K
174 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 760 °C
1400 °F
Significant oxidation resistance to this temp.
Component Elements Properties Metric English Comments
Carbon, C 0.010 %
0.010 %
Chromium, Cr 11 %
11 %
Iron, Fe 88 %
88 %
as balance
Manganese, Mn 0.30 %
0.30 %
Nickel, Ni 0.25 %
0.25 %
Niobium, Nb (Columbium, Cb) 0.15 %
0.15 %
Nitrogen, N 0.012 %
0.012 %
Phosphorous, P 0.023 %
0.023 %
Silicon, Si 0.41 %
0.41 %
Sulfur, S 0.0010 %
0.0010 %
Titanium, Ti 0.17 %
0.17 %
(Ti + Nb) = 0.08 + 8 * (C+N) min.
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000600 ohm-cm
0.0000600 ohm-cm
Curie Temperature 732 °C
1350 °F
Copyright © lookpolymers.com All Rights Reserved