Chicago Extruded Metals BioBrass® UNS C64200 Aluminum Bronze

Category Metal , Nonferrous Metal , Copper Alloy , Bronze
Manufacturer Chicago Extruded Metals (CXM)
Trade Name BioBrass®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chicago Extruded Metals BioBrass® UNS C64200 Aluminum Bronze.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Finished product available as bar, rod, forged, or shapes.Chicago Extruded Metal temper codes: H02, M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metals
Physical Properties Metric English Comments
Density 7.70 g/cc
0.278 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 77 - 98
77 - 98
Tensile Strength 517 - 703 MPa
75000 - 102000 psi
Tensile Strength, Yield 241 - 469 MPa
35000 - 68000 psi
Elongation at Break 22 - 32 %
22 - 32 %
Thermal Properties Metric English Comments
Thermal Conductivity 104 W/m-K
720 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Aluminum, Al 6.3 - 7.6 %
6.3 - 7.6 %
Copper, Cu >= 88.5 %
>= 88.5 %
as balance
Iron, Fe <= 0.30 %
<= 0.30 %
Lead, Pb <= 0.050 %
<= 0.050 %
Manganese, Mn <= 0.10 %
<= 0.10 %
Nickel, Ni <= 0.25 %
<= 0.25 %
Other, total 0.50 %
0.50 %
Silicon, Si 1.5 - 2.2 %
1.5 - 2.2 %
Tin, Sn <= 0.20 %
<= 0.20 %
Zinc, Zn <= 0.30 %
<= 0.30 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000216 ohm-cm
0.0000216 ohm-cm