Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 276 - 345 MPa @Strain 0.200 % |
40000 - 50000 psi @Strain 0.200 % |
|
Materion BrushCAST® 20C High Strength Casting Alloy (As Cast) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Yield | 276 - 345 MPa @Strain 0.200 % |
40000 - 50000 psi @Strain 0.200 % |
|
Materion BrushCAST® 21C High Strength Casting Alloy (As Cast) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Yield | 170 - 345 MPa | 24700 - 50000 psi | |
Materion Brush 1915™ AT Temper Rod Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe.. |
|||
Tensile Strength, Yield | 276 - 345 MPa @Strain 0.200 % |
40000 - 50000 psi @Strain 0.200 % |
|
Materion BrushCAST® 20CT Fine Grain Casting Alloy (As Cast) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Yield | 207 - 345 MPa @Strain 0.200 % |
30000 - 50000 psi @Strain 0.200 % |
Annealed temper |
Special Metals INCONEL® 601GC® Nickel Superalloy Data provided by the manufacturer, Special Metals. |
|||
Tensile Strength, Yield | 283 - 345 MPa | 41000 - 50000 psi | 0.2% offset |
Eagle Brass 110 EPT COPPER, Hard Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of .. |
|||
Tensile Strength, Yield | 276 - 345 MPa | 40000 - 50000 psi | 0.2% offset |
Eagle Brass 151 ZHC® COPPER, 1/2 Hard Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c.. |
|||
Tensile Strength, Yield | 241 - 345 MPa | 35000 - 50000 psi | 0.2% offset |
Eagle Brass 240 Low Brass, 1/2 Hard CDA 240 has excellent ductility, corrosion resistance and strength which allows it to be deep drawn, etched, stamped, blanked and bent. Typical uses include musical instruments, battery caps, flexib.. |
|||
Tensile Strength, Yield | 138 - 345 MPa | 20000 - 50000 psi | 0.2% offset |
Eagle Brass 511 Phosphor Bronzes 4%, 1/4 Hard 511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge.. |
|||
Tensile Strength, Yield | 103 - 345 MPa | 15000 - 50000 psi | |
Chicago Extruded Metals UNS C34500 Copper-Zinc-Lead Alloy Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available in rods.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals |
|||
Tensile Strength, Yield | 283 - 345 MPa | 41000 - 50000 psi | 0.2% offset |
Eagle Brass 101 OFE COPPER (Certified), Hard Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information.. |
|||
Tensile Strength, Yield | 283 - 345 MPa | 41000 - 50000 psi | 0.2% offset |
Eagle Brass 102 OF COPPER (Non-Certified), Hard Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an.. |
|||
Tensile Strength, Yield | 317 - 345 MPa | 46000 - 50000 psi | |
Chicago Extruded Metals BioBrass® CXM10 Lead-Free Alloy Finished product available in rods.Chicago Extruded Metal temper code: H02This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metals |
|||
Tensile Strength, Yield | 276 - 345 MPa @Strain 0.200 % |
40000 - 50000 psi @Strain 0.200 % |
|
AK Steel 436L ULTRA FORM® Ferritic Stainless Steel AK Steel’s 436L ULTRA FORM® is a ferritic grade of stainless steel that outperforms Type 409 in oxidation resistance and corrosion testing. The addition of molybdenum enhances pitting resistance w.. |