Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 170 MPa | 24700 psi | ASTM D638 |
NYCOA 27/300I Glass Filled Nylon 6 30% glass filled, flame retardant to UL 94 V-0 nylon 6Information provided by NYCOA, Inc. |
|||
Tensile Strength, Yield | 170 MPa | 24700 psi | ISO 527-1/2 |
Radici Radilon® SRV300 (dry) Nylon 6 Glass-fiber reinforcedInformation provided by Radici group. |
|||
Tensile Strength, Yield | 170 MPa | 24700 psi | ISO 527, ASTM D638 |
Nilit Nilamid A3 H G6 General Purpose 30% Glass Reinforced PA66 Description: Nilamid A3 H G6 is a general purpose 30% glass fiber reinforced NYLON 66 that gives an excellent combination of tensile strength, stiffness and impact strength. It is one of the most wi.. |
|||
Tensile Strength, Yield | 170 - 310 MPa @Strain 0.200 % |
24700 - 45000 psi @Strain 0.200 % |
|
Kobe Steel KS40 Commercially Pure Titanium, ASTM Gr. 1, Annealed Nominal Composition: Ti-Fe-OApplications: PHE, press formed parts, roofs, walls Features: Excellent formability, Excellent corrosion resistanceInformation provided by Kobe Steel |
|||
Tensile Strength, Yield | 170 - 310 MPa @Strain 0.200 % |
24700 - 45000 psi @Strain 0.200 % |
|
Kobe Steel KS40S Commercially Pure Titanium, ASTM Gr. 1, Annealed Nominal Composition: Ti-Fe-OApplications: PHE, press formed parts, roofs, walls Features: Excellent formability, Excellent corrosion resistanceInformation provided by Kobe Steel |
|||
Tensile Strength, Yield | 170 - 380 MPa | 24700 - 55100 psi | |
Materion Brush 1915â„¢ Hard Temper Wire, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Tensile Strength, Yield | >= 170 MPa | >= 24700 psi | |
MetalTek C86500 Low Tensile Manganese Bronze High aqueous and atmospheric corrosion resistance, moderate strength and conductivity.Applications: Valves, pumps, pipe fittings, electric terminal ends.Information provided by MetalTekCast UNS C836.. |
|||
Tensile Strength, Yield | >= 170 MPa | >= 24700 psi | |
MetalTek MTEK 175 Low Iron Cast UNS C95300 Aluminum Bronze Versatile alloy with high strength, good ductility, unusual toughness, plus exceptional wear resistance. Aluminum Bronze heat treated to higher mechanical properties where necessary.Information prov.. |
|||
Tensile Strength, Yield | >= 170 MPa | >= 24700 psi | |
MetalTek MTEK 20-32Nb Cast UNS N08151 Heat Resistant Stainless Steel Information provided by MetalTek |
|||
Tensile Strength, Yield | >= 170 MPa | >= 24700 psi | |
MetalTek MTEK 90-10 UNS C96200 Nickel-Copper Alloy Information provided by MetalTek |
|||
Tensile Strength, Yield | >= 170 MPa | >= 24700 psi | |
MetalTek MTEK Super 20-32Nb Cast UNS N08151 Heat Resistant Stainless Steel Information provided by MetalTek |
|||
Tensile Strength, Yield | >= 170 MPa | >= 24700 psi | |
MetalTek MTEK 65+Ni UNS C91600 Gear Bronze Copper-tin alloy with high tensile, yield and compressive strength as well as wear resistance.Applications: Worm gears, steel mill nutsInformation provided by MetalTekCast UNS C91600; Cast Grade C91.. |
|||
Tensile Strength, Yield | 170 MPa @Strain 0.200 %, Temperature 650 °C |
24700 psi @Strain 0.200 %, Temperature 1200 °F |
|
Haynes HR-120® alloy, solution heat-treated plate Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Tensile Strength, Yield | 170 MPa | 24700 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 2410EPR PEI (Asia Pacific) 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Tensile Strength, Yield | 170 MPa | 24700 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 2410EPR PEI (Europe-Africa-Middle East) 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. Resin is RoHS compliant. UL94 V0 listing. |
|||
Tensile Strength, Yield | 170 MPa @Temperature 425 °C |
24700 psi @Temperature 797 °F |
Annealed prior to test |
Special Metals MONEL® Alloy 400 A nickel-copper alloy with high strength and excellent corrosion resistance in a range of media including sea water, hydrofluoric acid, sulfuric acid, and alkalis. Used for marine engineering, chem.. |
|||
Tensile Strength, Yield | 170 MPa | 24700 psi | ASTM-D638 |
Polyram Polytron A30B041 Nylon 66, 30% Long Fiber 30% LONG FIBER GLASS REINFORCED, PTFE LUBRICATED, UV STABILIZED BLACK NYLON 6.6 FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 170 MPa | 24700 psi | ASTM-D638 |
Polyram PlusTek RA304G6 Nylon 6.6, 30% Glass Fiber 30% glass fiber reinforced, heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 170 MPa | 24700 psi | ASTM D638, ISO R527 |
EPICHEM Epinyl PA 66 GF 30 Polyamide 66, 30% Glass Characteristics: 30% glass fibre filled |
|||
Tensile Strength, Yield | 170 MPa | 24700 psi | ISO 527 |
Eurostar Star L PA6 30V D31 PA6, Glass Filled, Injection Molding Star L PA6 30V D31 is a Molybdenum Disulfide Lubricated, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Strength, Yield | 170 MPa | 24700 psi | 5 mm/min; ISO 527 |
Eurostar Staramide RF006EU PA66/6, Glass Fiber Filled, Injection Molded Staramide RF006EU is an UV stabilized, Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as Staramide 66C 30V S4)Information provided by Eurostar. |
|||
Tensile Strength, Yield | 170 MPa | 24700 psi | ASTM D638 |
E-Polymers TEKAMID® TB120G30 , 30% Glass Fiber Reinforced PA6, DAM 30% Glass Fiber Reinforced, Good impact resistanceInformation provided by E-Polymers Co. Ltd. |
|||
Tensile Strength, Yield | >= 170 MPa | >= 24700 psi | |
AK Steel Grade 25 Cold Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Tensile Strength, Yield | 170 MPa | 24700 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® R543H NT Nylon 66, 43% Glass Reinforced, Conditioned Vydyne® R543H NT is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
Tensile Strength, Yield | 170 MPa | 24700 psi | 50 mm/min; ISO 527-1/-2 |
BASF Ultramid® KR 4355 G5 BK 00564 25% Glass Filled PA6/6T (Conditioned) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Tensile Strength, Yield | 170 - 360 MPa | 24700 - 52200 psi | |
ArcelorMittal 11 High formability steel for drawing, Hot rolled Available in the following: uncoated (DD11) Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used extensively in the au.. |
|||
Tensile Strength, Yield | >= 170 MPa | >= 24700 psi | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, Annealed (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Tensile Strength, Yield | >= 170 MPa @Strain 0.200 % |
>= 24700 psi @Strain 0.200 % |
Annealed; Min required by ASTM A 240 and ASME SA-240 |
ATI Allegheny Ludlum Type 316L Stainless Steel, UNS S31603 This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels .. |
|||
Tensile Strength, Yield | 170 MPa | 24700 psi | ASTM D638 |
Techmer ES Luriblend® PPA GF30 TL15 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, High Heat Resistance and Low .. |
|||
Tensile Strength, Yield | >= 170 MPa @Strain 0.200 % |
>= 24700 psi @Strain 0.200 % |
|
Industeel SIRIUS 800 H Heat Resistant Alloy Description: The SIRIUS® 800, H and H+ grades are three variants of a high chromium and nickel austenitic alloy which combines good corrosion and creep resistance. SIRIUS® 800 is employed at tempe.. |