Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Alathon® M4661 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer LyondellBasell (former Equistar)
Trade Name Alathon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Alathon® M4661 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsALATHON M 4661, formerly known as LYHD 060, exhibits excellent impact, warp and environmental stress crack resistance. Typical applications are closures, institutional seating and consumer durables. Through precise control of the molecular weight distribution M 4661 shows enhanced processability for a product with this melt index.Regulatory StatusM 4661 meets the requirements of the Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food..." Specific limitations or conditions of use may apply. Contact your Equistar polyethylene sales representative for more information.Processing TechniquesSpecific recommendations for processing M 4661 can only be made when the processing conditions, equipment and end use are known. For further suggestions, please contact your Equistar sales representative.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.946 g/cc
0.0342 lb/in³
ASTM D1505
Melt Flow 6.1 g/10 min
6.1 g/10 min
ASTM D1238
Spiral Flow 24.4 cm
9.60 in
Measures the number on inches of flow produced when molten resin is injected into a long, spiral channel (0.625” insert), at a constant injection pressure of 1000 psi with a melt temperature of 440°F.; Equistar
Mechanical Properties Metric English Comments
Hardness, Shore D 68
68
ASTM D2240
Tensile Strength at Break 15.2 MPa
2200 psi
Crosshead speed - 2" min; ASTM D638
Tensile Strength, Yield 22.8 MPa
3310 psi
Crosshead speed - 2" min; ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
1% Secant Modulus 896 MPa
130000 psi
Crosshead speed - 0.5" min; ASTM D790
2% Secant Modulus 0.758 GPa
110 ksi
Crosshead speed - 0.5" min; ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 60.0 °C
140 °F
ASTM D648
Vicat Softening Point 124 °C
255 °F
ASTM D1525
Brittleness Temperature <= -76.0 °C
<= -105 °F
ASTM D746