Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Elastocon TPE Technologies Elastocon® SMR1000 Thermoplastic Polyolefin Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer Elastocon TPE Technologies
Trade Name Elastocon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Elastocon TPE Technologies Elastocon® SMR1000 Thermoplastic Polyolefin Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elastocon® SMR1000 thermoplastic polyolefin elastomer has been developed for applications that require impact resistance and a high gloss scratch and mar resistant surface finish. Elastocon® SMR1000 is FDA compliant and well suited for consumer goods and industrial applications requiring U.V. stability. Elastocon® SMR1000 eliminates stress whitening.Information provided by Elastocon® TPE Technologies
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.015 - 0.025 cm/cm
0.015 - 0.025 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 22.8 MPa
3310 psi
ASTM D412
Elongation at Break 243 %
243 %
ASTM D412
100% Modulus 0.0147 GPa
2.13 ksi
ASTM D412
Processing Properties Metric English Comments
Rear Barrel Temperature 200 - 225 °C
392 - 437 °F
Front Barrel Temperature 200 - 230 °C
392 - 446 °F
Nozzle Temperature 200 - 235 °C
392 - 455 °F
Mold Temperature 21.0 - 49.0 °C
69.8 - 120 °F
Back Pressure 0.689 - 1.38 MPa
99.9 - 200 psi
Descriptive Properties Value Comments
Injection Velocity (mm/sec) Fast
Copyright © lookpolymers.com All Rights Reserved