Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 32.8 MPa | 4750 psi | 2 in per min; ASTM D638 |
Network Polymers NPP 25-1503 G10 Description: Glass Reinforced PolypropyleneInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 32.8 MPa | 4750 psi | (2 in/min); ASTM D638 |
Phillips 66 COPYLENE® CM003 Polypropylene Impact Copolymer CM003 is a fractional melt flow impact copolymer with a barefoot additive package which is specially formulated to excel in extrusion processes.Applications: Extrusion ProcessesInformation provided .. |
|||
Tensile Strength, Yield | 32.8 MPa | 4750 psi | 2 in/min; ASTM D638 |
Phillips 66 COPYLENE® CM040LN Polypropylene, Impact Copolymer, Thermoforming COPYLENE™ CM040LN is an impact copolymer specially designed for excellent processing in thermoforming applications and is formulated with antistat and nucleation. Applications: Thermoforming, Injec.. |
|||
Tensile Strength, Yield | 32.8 MPa | 4750 psi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 1.0 PHR MBT Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tensile Strength, Yield | 32.8 MPa | 4750 psi | Type I, 2 in/min; ASTM D638 |
M. Holland Company PP400 Polypropylene Homopolymer Features: Medium Flow, General PurposeUses: Closures, Food Containers, Household Goods, VialsApprovals: FDA 21 CFR 177.1520Processing Method: Injection MoldingInformation provided by M. Holland. |
|||
Tensile Strength, Yield | 32.8 MPa @Temperature 23.0 °C |
4760 psi @Temperature 73.4 °F |
ASTM D638 |
Ineos H36G-00 Polypropylene Homopolymer This is a high flow rate homopolymer. This material is designed for fiber spinning and spun bonded processes. It meets the requirements of the U.S. Food and Drug Administration as specified in 21 .. |
|||
Tensile Strength, Yield | 32.8 MPa | 4750 psi | ASTM D638 |
Techmer ES HiFill® HDPE TM40 40% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 40% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 32.8 MPa | 4750 psi | ASTM D638 |
Washington Penn Homopolymer Polypropylene Grades are available to meet FDA food and drug packaging requirements. These products have excellent mold detail and surface reproduction with fast set-up times. They are also available in an array .. |
|||
Tensile Strength, Yield | 32.8 MPa | 4750 psi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 1.0 PHR MBT Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tensile Strength, Yield | 32.8 MPa | 4750 psi | 20 in/min; ASTM D638 |
ExxonMobil PP9074MED Polypropylene Homopolymer Product Description: A highly clarified random copolymer resin designed for injection molding of medical devices suitable for sterilization by high energy radiation.Availability: Europe and North A.. |
|||
Tensile Strength, Yield | 32.8 MPa | 4750 psi | ASTM D-638 |
Bapolene® 4017 Polypropylene Bapolene 4017 is a homopolymer polypropylene with outstanding modulus. It complies with FDA 21 CFR1777.1520.Applications: Strapping, profile extrusion, and general purpose.Bapolene® and Bapolan® .. |