Material Notes:
Product Description: A highly clarified random copolymer resin designed for injection molding of medical devices suitable for sterilization by high energy radiation.Availability: Europe and North America Features:Controlled RheologyE-beam SterilizableEthylene Oxide SterilizableHigh ClarityRadiation (Gamma) ResistantRadiation Sterilizable Uses: Hypodermic Syringe PartsLabwareMedical PackagingMedical/Healthcare ApplicationsProcessing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ExxonMobil Method
Melt Flow 24 g/10 min

@Load 2.16 kg,
Temperature 230 °C
24 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 17.2 MPa
2500 psi
20 in/min; ASTM D638
Tensile Strength, Yield 32.8 MPa
4750 psi
20 in/min; ASTM D638
Elongation at Break 51 %
51 %
20 in/min; ASTM D638
Elongation at Yield 13 %
13 %
20 in/min; ASTM D638
Flexural Modulus, 1% Secant 1050 MPa
153000 psi
0.05 in/min; ASTM D790A
Izod Impact, Notched 0.641 J/cm
1.20 ft-lb/in
ASTM D256A
Gardner Impact 23.6 J

@Thickness 3.17 mm,
Temperature -28.9 °C
17.4 ft-lb

@Thickness 0.125 in,
Temperature -20.0 °F
Geometry GC; ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C
167 °F
ASTM D648
Optical Properties Metric English Comments
Haze 8.6 %
8.6 %
ASTM D1003