Material Notes:
Bapolene 4017 is a homopolymer polypropylene with outstanding modulus. It complies with FDA 21 CFR1777.1520.Applications: Strapping, profile extrusion, and general purpose.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D-1505
Melt Flow 1.3 g/10 min
1.3 g/10 min
ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D-785
Tensile Strength, Yield 32.8 MPa
4750 psi
ASTM D-638
Elongation at Yield 10 %
10 %
ASTM D-638
Flexural Modulus, 1% Secant 1272 MPa
184500 psi
ASTM D-790
Izod Impact, Notched 0.270 J/cm
0.506 ft-lb/in
ASTM D-785
Descriptive Properties Value Comments
Process Extrusion
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Copyright © lookpolymers.com All Rights Reserved