Phillips 66 COPYLENE® CM040LN Polypropylene, Impact Copolymer, Thermoforming

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Phillips 66
Trade Name COPYLENE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Phillips 66 COPYLENE® CM040LN Polypropylene, Impact Copolymer, Thermoforming.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
COPYLENE™ CM040LN is an impact copolymer specially designed for excellent processing in thermoforming applications and is formulated with antistat and nucleation. Applications: Thermoforming, Injection Molding.Information provided by Phillips 66.
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
ASTM D792
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.8 MPa
4750 psi
2 in/min; ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Modulus 1.52 GPa
220 ksi
0.05 in/min; 1% secant; Procedure A; ASTM D790
Izod Impact, Notched 0.908 J/cm

@Temperature 23.0 °C
1.70 ft-lb/in

@Temperature 73.4 °F
Method A; ASTM D256
Descriptive Properties Value Comments
Process Injection Molding
Thermoforming