Washington Penn Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Washington Penn
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Washington Penn Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Grades are available to meet FDA food and drug packaging requirements. These products have excellent mold detail and surface reproduction with fast set-up times. They are also available in an array of colors.Information provided by Washington Penn Plastic Co.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Filler Content 0.00 %
0.00 %
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.8 MPa
4750 psi
ASTM D638
Elongation at Break 540 %
540 %
ASTM D638
Elongation at Yield 20 %
20 %
ASTM D638
Flexural Modulus 1.41 GPa
205 ksi
1% Secant; ASTM D790
1.48 GPa
215 ksi
Tangent; ASTM D790
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
ASTM D256
Gardner Impact 6.33 J

@Temperature 23.0 °C
4.67 ft-lb

@Temperature 73.4 °F
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 82.2 °C
180 °F
ASTM D648