Material Notes:
Grade R35C-02 is a high clarity, lubricated random copolymer with a high flow rate. This material is designed for high-speed injection molding of medium- to thin-walled parts requiring excellent clarity, fast cycle times, and ease of denesting. Finished parts made with R35C-02 will exhibit a bluish hue giving a look of enhanced clarity. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.Applications:Medium- to thin-walled injection molding of multi-cavity partsHousewares and consumer products – especially storage bins, containers and cupsAudio and video media rigid packagingBenefits:High flow rateFast cycling timeExcellent clarityExcellent mold release and denesting of partsGood impact resistanceInformation provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 83.5
83.5
ASTM D785
Tensile Strength, Yield 29.6 MPa
4300 psi
ASTM D638
Elongation at Break >= 200 %
>= 200 %
ASTM D638
Flexural Modulus 1.05 GPa
153 ksi
ASTM D790A
Izod Impact, Notched 0.603 J/cm
1.13 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 77.0 °C
171 °F
ASTM D648
Optical Properties Metric English Comments
Haze 14.3 %
14.3 %
As molded, 50-mil plaque, % Diffuse Transmittance; ASTM D1003
16.4 %
16.4 %
ASTM standard conditioning, 50-mil plaque, % Diffuse Transmittance; ASTM D1003
Descriptive Properties Value Comments
Process Injection Molding
Region Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution