Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 29.6 MPa | 4290 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ HTX M6307 Polyvinyl Chloride Alloy (PVC Alloy) Information provided by PolyOne |
|||
Tensile Strength, Yield | 29.6 MPa | 4290 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ DP 9052-3-1000 Polyethylene, High Density (HDPE) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Tensile Strength, Yield | 29.6 MPa | 4290 psi | ASTM D638 |
Albis Plastics Cellulose Acetate CA700 , Unreinforced, 29% Plasticizer
(discontinued **) Amorphous Cellulose Acetate (CA)Characteristics: Chemical Resistance, Toughness, Strength, Hardness, Gloss, Clarity and "Feel"Applications: Tool Handles, Optical Products, Toys and Sheet ProductsPro.. |
|||
Tensile Strength, Yield | 29.6 MPa | 4290 psi | ASTM Data |
Styron Magnum™ 213 ABS, General Purpose MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 29.6 MPa | 4290 psi | 2 in/min; ASTM D638 |
A. Schulman POLYFORT™ PP 3052UX Impact Resistant Copolymer DescriptionPolyfort® PP 3052UX is a UV stabilized extra high flow impact resistant copolymer with a relatively high stiffness.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 29.6 MPa | 4290 psi | 2 in/min; ASTM D638 |
A. Schulman POLYFORT™ PP 3052UX Impact Resistant Copolymer DescriptionPolyfort® PP 3052UX is a UV stabilized extra high flow impact resistant copolymer with a relatively high stiffness.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 29.6 MPa | 4290 psi | 2 in/min; ASTM D638 |
A. Schulman POLYFORT™ PP 3052UX Impact Resistant Copolymer DescriptionPolyfort® PP 3052UX is a UV stabilized extra high flow impact resistant copolymer with a relatively high stiffness.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 29.6 MPa | 4290 psi | 2 in/min; ASTM D638 |
A. Schulman POLYFORT™ PP 3052UX Impact Resistant Copolymer DescriptionPolyfort® PP 3052UX is a UV stabilized extra high flow impact resistant copolymer with a relatively high stiffness.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 29.6 MPa | 4290 psi | ASTM D638 |
Eastman Tenite Acetate 105E1R26033 Clear, Trsp Cellulose Acetate Plasticizer 29%. Weight loss on heating = 2.6% per ASTM D 707. Soluble matter loss = 0.4% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Yield | 29.6 MPa | 4290 psi | ASTM D638 |
Chevron Phillips Marlex® 9512H - 9513H High Performance Series HDPE Blow Molding Resin Resin Type: linear copolymerCharacteristics: excellent physical properties, medium molecular weight distribution, wide range of processing conditions, good flow for injection blow molding applicatio.. |
|||
Tensile Strength, Yield | 29.6 MPa | 4290 psi | ASTM D638 |
Dow R792-35RNA Polypropylene Random Copolymer Resin OverviewControlled rheology productConsistent processabilityContains clarifying additiveContains an antistatic additiveComplies with U.S. FDA 21 CFR 177.1520 (c)3.1a, Canadian HPFB No ObjectionDOW R.. |
|||
Tensile Strength, Yield | 29.6 MPa | 4290 psi | 2 in/min; ASTM D638 |
A. Schulman POLYFORT™ PP 3052UX Impact Resistant Copolymer DescriptionPolyfort® PP 3052UX is a UV stabilized extra high flow impact resistant copolymer with a relatively high stiffness.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 29.6 MPa | 4290 psi | 2 in/min; ASTM D638 |
A. Schulman POLYFORT™ PP 3052UX Impact Resistant Copolymer DescriptionPolyfort® PP 3052UX is a UV stabilized extra high flow impact resistant copolymer with a relatively high stiffness.Information provided by A. Schulman. |