Material Notes:
Product Description: A specialty thermoplastic olefin resin with good flow, cold temperature impact resistance, low CLTE, medium shrinkage and excellent paintability for automotive exterior applications.Availability: North America Features: DuctileGood UV ResistanceHigh FlowLow Temperature Impact ResistancePaintableUses: Automotive ApplicationsAutomotive BumperAutomotive Exterior TrimAutomotive Specifications: GM GM7001 EP and GM GMP.E/P.133 Processing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ISO 1183
Melt Flow 24 g/10 min

@Load 2.16 kg,
Temperature 230 °C
24 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.5 MPa
2540 psi
ISO 527-2/50
Flexural Modulus 1.07 GPa
155 ksi
Secant, 0.079 in/min; ISO 178
Dart Drop, Total Energy 16.4 J

@Thickness 3.20 mm,
Temperature 22.8 °C
12.1 ft-lb

@Thickness 0.126 in,
Temperature 73.0 °F
Energy to Peak Force, Ductile Failure, 7.33 ft/sec; ASTM D3763
26.2 J

@Thickness 3.20 mm,
Temperature -30.0 °C
19.3 ft-lb

@Thickness 0.126 in,
Temperature -22.0 °F
Energy to Peak Force, Ductile Failure, 7.33 ft/sec; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 0.774 µm/m-°C

@Temperature -30.0 - 100 °C
0.430 µin/in-°F

@Temperature -22.0 - 212 °F
ASTM E831