Ashley Polymers Ashlene® PE126 PET Polyester, 30% Glass Reinforced

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), 30% Glass Reinforced
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® PE126 PET Polyester, 30% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PET Polyester, with 30% glass reinforcement.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.55 g/cc
0.0560 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Yield 152 MPa
22000 psi
ASTM D638
Elongation at Break 2.2 %
2.2 %
Flexural Strength 228 MPa
33100 psi
ASTM D790
Flexural Modulus 8.60 GPa
1250 ksi
ASTM D790
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 245 °C
473 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 224 °C
435 °F
ASTM D648
Electrical Properties Metric English Comments
Dielectric Constant 3.5

@Frequency 1e+6 Hz
3.5

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 22.0 kV/mm

@Thickness 3.20 mm
559 kV/in

@Thickness 0.126 in
Short Time; ASTM D149
Dissipation Factor 0.021

@Frequency 1e+6 Hz
0.021

@Frequency 1e+6 Hz
ASTM D150