Clariant Renol BR2084 Nylon 66, 33% Glass Fiber, PTFE Lubricated

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled , Nylon 66, PTFE Filled
Manufacturer Clariant
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Clariant Renol BR2084 Nylon 66, 33% Glass Fiber, PTFE Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Clariant Masterbatches
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 152 MPa
22000 psi
ASTM D638
Elongation at Yield 3.0 %
3.0 %
ASTM D638
Flexural Yield Strength 228 MPa
33000 psi
ASTM D790
Flexural Modulus 8.96 GPa
1300 ksi
ASTM D790
Izod Impact, Notched 0.641 J/cm

@Temperature 22.8 °C
1.20 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 260 - 293 °C
500 - 560 °F
Mold Temperature 93.3 - 121 °C
200 - 250 °F
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
8.27 - 13.8 MPa
1200 - 2000 psi
Initial
Back Pressure 0.000 - 0.345 MPa
0.000 - 50.0 psi
Shot Size 30 - 80 %
30 - 80 %
Screw Speed 20 - 100 rpm
20 - 100 rpm
Users viewing this material also viewed the following: