Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
ASTM D2240
Tensile Strength, Ultimate 22.4 MPa
3250 psi
ASTM D412
Tensile Strength, Yield 2.90 MPa
420 psi
at 100%; ASTM D412
Elongation at Break 575 %
575 %
ASTM D412
Tear Strength 42.1 kN/m
240 pli
die C; ASTM D624
Compression Set 45 - 50 %
45 - 50 %
ASTM D395