Material Notes:
A medium flow general purpose injection molding resin with good gloss, toughness and good chemical resistance. This product meets FDA standards for food contact applications.Applications: Caps and closures, toys, novelties, color concentrates, and housewares.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D1505
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 50
50
ASTM D-2240
Tensile Strength, Yield 10.3 MPa
1490 psi
2 in/min (50 mm/min); ASTM D638
Elongation at Break 350 %
350 %
2 in/min (50 mm/min); ASTM D638
Modulus of Elasticity 0.221 GPa
32.1 ksi
ASTM D-638
Flexural Modulus 0.210 GPa
30.5 ksi
Tangent Method 1; ASTM D-790
Izod Impact, Notched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 99.0 °C
210 °F
ASTM D1525
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D-746
Descriptive Properties Value Comments
Process Injection Molding
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following: