Polymer Property : Film Tensile Strength at Break, MD = 55.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 55.0 MPa
7980 psi
ASTM D882
SABIC F01552 High Density Polyethylene for Blown Film
Product Description: F01552 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh..
Film Tensile Strength at Break, MD 55.0 MPa
7980 psi
Premix Thermoplastics PREFLEX E12.5 Polyphenylene Ether (PPO/PPE)
PREFLEX films combine outstanding dielectric properties, good heat stability, low water absorption and chemical resistance in a way not available before. Also rigid boards made of the same material ..
Film Tensile Strength at Break, MD 55.0 MPa
7980 psi
ASTM D882
Chevron Phillips HiD® 9632 HDPE Blown Film Resin  (discontinued **)
Characteristics: Copolymerization Enhances Film Toughness, Excellent Film Drawdown Ideally Suited for Thin Films Production, Lower Melt Index (Higher Molecular Weight) Results in Increased Film Stre..
Film Tensile Strength at Break, MD 55.0 MPa
7980 psi
ASTM D882
Reliance Industries Relene F46003 Polyethylene
Relene F46003 is a High Density Polyethylene grade suitable for producing blown parts with superior stiffness and barrier properties. It is recommended for making liners and coextruded film structu..
Film Tensile Strength at Break, MD 55.0 MPa
7980 psi
ASTM D882
Reliance Industries Relene F56003 Polyethylene
Relene F56003 is a High Density Polyethylene grade suitable for producing blown parts with excellent drawdown and paper like feel. It is recommended for making carrier bags and coextruded film stru..
Film Tensile Strength at Break, MD <= 55.0 MPa
<= 7980 psi
ISO 527-1.3
Iran Petrochemical (PCC) MF3313 High Density Polyethylene
MF3313 is a high molecular weight high density polyethylene . Applications: extrusion, film, blown, bags, and density modifies.Information provided by Iran Petrochemical Commercial Co.
Film Tensile Strength at Break, MD 55.0 MPa
7980 psi
ISO 527-3
Borealis Borstar® FB2230 LLDPE for Film
Borstar BF2230 is a high molecular weight low density polyethylene film grade combining good and flexible extrusion behavior, excellent draw down and superior mechanical properties. Film made from ..
Film Tensile Strength at Break, MD 55.0 MPa
7980 psi
ISO 527-3
Topas Advanced Polymers TOPAS® 6013F-04 Cyclic Olefin Copolymer (COC)
TOPAS® 6013F-04 is a high temperature, general purpose film extrusion grade. It is a high clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, thermoformability and p..
Film Tensile Strength at Break, MD 55.0 MPa
7980 psi
ISO 527-3
Topas Advanced Polymers TOPAS® 9506F-500 Cyclic Olefin Copolymer (COC)
TOPAS® 9506F-500 is a high clarity extrusion grade for use in shrink, food and medical packaging as either a discrete layer in multilayer film or in blends with polyethylene. It is designed to del..
Film Tensile Strength at Break, MD 55.0 MPa
7980 psi
ISO 527-3
Topas Advanced Polymers TOPAS® 8007F-400 Cyclic Olefin Copolymer (COC)
TOPAS® 8007F-400 is a robust film extrusion grade designed for blending with polyethylene (PE). It is a moderate clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, ..
Film Tensile Strength at Break, MD 55.0 MPa
7980 psi
ISO 527-3
Total PPR 6280 Random Copolymer Polypropylene, Cast Film Extrusion Grade
Total Petrochemicals PPR 6280 is a random copolymer polypropylene with a melt flow index of 7 g/10 min suitable for the cast extrusion of films with outstanding optical properties and easy heat weld..
Film Tensile Strength at Break, MD 55.0 MPa
7980 psi
Blown Film at 1 mil; ASTM D-882
Chevron Phillips MarFlex® 7308DK Polyethylene; LLDPE
Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: Excellent processingIncreased stiffnessGood toughnessUse alone or in blends with LDPE or HD..
Film Tensile Strength at Break, MD 55.0 MPa
7980 psi
Blown Film at 1 mil; ASTM D-882
Chevron Phillips MarFlex® 7308DL Polyethylene; LLDPE
Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: Excellent processingIncreased stiffnessGood toughnessUse alone or in blends with LDPE or HD..
Film Tensile Strength at Break, MD 55.0 MPa
7980 psi
Blown Film at 1 mil; ASTM D-882
Chevron Phillips MarFlex® 7308FK Polyethylene; LLDPE
Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: Excellent processabilityIncreased stiffnessGood toughnessUse alone or in blends with LDPE o..
Film Tensile Strength at Break, MD >= 55.0 MPa
>= 7980 psi
55 N/10mm
Dr. D. Mueller Flexiso® DMD FI 14010 00100 Polyester Electrical Insulation
Structure: Flexiso® DMD, FI 14010 00100 is a flexible three layer material, consisting of a layer of polyester film, of which both sides have a layer of polyester fleece fabric and is coated with ..
Film Tensile Strength at Break, MD 55.0 MPa
7980 psi
ASTM D882
Dow AFFINITY™ PL 1840 Polyolefin Plastomer
AFFINITY® PL 1840 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide blown film products with low temperature sealability, excellent puncture resistance, outstanding blown f..
Film Tensile Strength at Break, MD 55.0 MPa
7980 psi
ISO 527-3
Polimeri Europa Eraclene® FA 506 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion
Eraclene FA 506 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Its broad molecular weight distribution and density successfully c..