Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow AFFINITY™ PL 1840 Polyolefin Plastomer

Category Polymer , Film , Thermoplastic , Elastomer, TPE
Manufacturer Dow Chemical
Trade Name AFFINITY™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow AFFINITY™ PL 1840 Polyolefin Plastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AFFINITY® PL 1840 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide blown film products with low temperature sealability, excellent puncture resistance, outstanding blown film optics, and good organoleptic properties. AFFINITY PL 1840 polymer has good clarity and toughness. It finds applications as sealant layer in multilayer film structures, and in liquid and dry food pouch packaging structures. It also offers excellent performance for profile extrusion of tubing. AFFINITY PL 1840 polymer has excellent compatibility with other polyolefins, allowing efficient blending and coextrusion. It complies with FDA regulation 21 CFR 177.1520c3.1b, which allows for its use in direct food contact applications.Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.908 g/cc
0.0328 lb/in³
Melt Flow 1.0 g/10 min

@Load 2.16 kg
1.0 g/10 min

@Load 4.76 lb
Melt flow ratio I10/I2 is 10.
Mechanical Properties Metric English Comments
Hardness, Shore D 94
94
Tensile Strength, Ultimate 15.6 MPa
2260 psi
Molded property
Tensile Strength, Yield 6.80 MPa
986 psi
Film Elongation at Break, MD 660 %
660 %
Film Elongation at Break, TD 730 %
730 %
Elongation at Break 360 %
360 %
Molded value
Flexural Modulus 0.141 GPa
20.5 ksi
Film Tensile Strength at Break, MD 55.0 MPa
7980 psi
ASTM D882
Film Tensile Strength at Break, TD 52.7 MPa
7640 psi
ASTM D882
Thermal Properties Metric English Comments
Vicat Softening Point 97.0 °C
207 °F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved