Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Film Tensile Strength at Yield, MD = 4500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 31.0 MPa
4500 psi
ASTM D882
SABIC F01552 High Density Polyethylene for Blown Film
Product Description: F01552 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh..
Film Tensile Strength at Yield, MD 31.0 MPa
4500 psi
ISO 527
Premix Thermoplastics PRE-ELEC® PE 1292
PRE-ELEC PE 1292 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129..
Film Tensile Strength at Yield, MD 31.0 - 39.3 MPa
4500 - 5700 psi
ASTM D882
Honeywell Halar® High Performance E-CTFE Film  (discontinued **)
Description: Halar® is a high performance Ethylene-Chlorotrifluoroethylene (E-CTFE) film with excellent mechanical, electrical and release properties. It is non-flammable, and has outstanding chem..
Film Tensile Strength at Yield, MD 31.0 MPa
4500 psi
ASTM D882
LyondellBasell Alathon® L4907 High Density Polyethylene
ApplicationsALATHON L 4907 is a high molecular weight high density copolymer with broad dimodal molecular weight distribution. This resin exhibits high density and stiffness and is designed for gro..
Film Tensile Strength at Yield, MD 31.0 MPa

@Thickness 0.0254 mm
4500 psi

@Thickness 0.00100 in
ASTM D882A
Total 9458 HDPE Film Grade
Medium molecular weight grade. Excellent bubble stability, good compatibility with LDPE and LLDPE, good heat resistance, high stiffness and tensile strength.Applications: Release liners, Stand-up ba..
Film Tensile Strength at Yield, MD 31.0 MPa
4500 psi
ISO 527-3
Total PPH 4026 Polypropylene Homopolymer, Film
Polypropylene PPH 4026 is a homopolymer polypropylene with a Melt Flow index of 3 g/10 min for the cast extrusion of films with outstanding stiffness and heat resistance.Polypropylene PPH 4026 is in..
Film Tensile Strength at Yield, MD 31.0 MPa
4500 psi
parallel; ISO 527-3
DSM Akulon® F130 PA6
Film Extrusion, Medium Viscosity
Film Tensile Strength at Yield, MD 31.0 MPa
4500 psi
parallel; ISO 527-3
DSM Akulon® F130-C PA6
Film Extrusion, Medium Viscosity, Lubricated
Film Tensile Strength at Yield, MD 31.0 MPa
4500 psi
parallel; ISO 527-3
DSM Akulon® F130-C2 PA6
Medium Viscosity, Film Extrusion, Lubricated
Film Tensile Strength at Yield, MD 31.0 MPa
4500 psi
parallel; ISO 527-3
DSM Akulon® F130-C3 PA6
Monofilament Grade, Extrusion Grade, Medium Viscosity, Lubricated
Film Tensile Strength at Yield, MD 31.0 MPa
4500 psi
parallel; ISO 527-3
DSM Akulon® F136 PA6
Very High Viscosity, Film Extrusion
Film Tensile Strength at Yield, MD 31.0 MPa
4500 psi
parallel; ISO 527-3
DSM Akulon® F136-C PA6
Film Extrusion, Very High Viscosity, Lubricated
Film Tensile Strength at Yield, MD 31.0 MPa
4500 psi
parallel; ISO 527-3
DSM Akulon® F136-C1 PA6
Very High Viscosity, Film Extrusion, Lubricated
Film Tensile Strength at Yield, MD 31.0 - 51.0 MPa
4500 - 7400 psi
Average value: 36.8 MPa Grade Count:12
Overview of materials for Nylon 6, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat..