Polymer Property : Film Tensile Strength at Yield, MD = 7400 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 37.9 - 51.0 MPa
5500 - 7400 psi
ASTM D882
Honeywell Capran® K Coated Nylon Film  (discontinued **)
Description: Capran® K is a PVdc coated nylon 6 film designed for food packaging applications where longer shelf life is required. This film exhibits good clarity, gloss, toughness, thermoformabil..
Film Tensile Strength at Yield, MD 37.9 - 51.0 MPa
5500 - 7400 psi
ASTM D882
Honeywell Capran® Nylon Film, Multipurpose Nylon 6 Film
Description: Capran® is a multipurpose nylon 6 film. Its physical properties are evenly distributed for optimum performance giving excellent resistance to flex cracking. It can be processed ove..
Film Tensile Strength at Yield, MD 31.0 - 51.0 MPa
4500 - 7400 psi
Average value: 36.8 MPa Grade Count:12
Overview of materials for Nylon 6, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat..