Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ensinger Tecamid® 6/6 Nylon (PA66)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer Ensinger
Trade Name Tecamid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecamid® 6/6 Nylon (PA66).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type 6/6 is a general purpose standard grade nylon. Extruded in natural and black. (Weather Resistant Black Grade is also available.)Information provided by Ensinger, Inc.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Water Absorption 1.2 %
1.2 %
at 24 hours; ASTM D570
Water Absorption at Saturation 8.5 %
8.5 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 90
90
ASTM D785
Tensile Strength, Yield 80.0 MPa
11600 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Tensile Modulus 2.41 GPa
350 ksi
ASTM D638
Flexural Strength 107 MPa
15500 psi
ASTM D790
Flexural Modulus 3.03 GPa
440 ksi
ASTM D790
Compressive Strength 34.5 MPa
5000 psi
ASTM D695
Izod Impact, Notched 0.587 J/cm
1.10 ft-lb/in
ASTM D256
Coefficient of Friction, Dynamic 0.26
0.26
40 psi, 50 fpm; ASTM D3702
K (wear) Factor 403 x 10-8 mm³/N-M
200 x 10-10 in³-min/ft-lb-hr
40 psi, 50 fpm; ASTM D3702
Thermal Properties Metric English Comments
CTE, linear 81.0 µm/m-°C

@Temperature 20.0 °C
45.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Specific Heat Capacity 1.67 J/g-°C
0.400 BTU/lb-°F
Melting Point 255 °C
491 °F
ASTM D2133
Maximum Service Temperature, Air 85.0 °C
185 °F
Long Term; ASTM UL746B
149 °C
300 °F
Intermittent
Deflection Temperature at 0.46 MPa (66 psi) 235 °C
455 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
ASTM D648
Flammability, UL94 V-2

@Thickness 3.00 mm
V-2

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Dielectric Constant 3.6

@Frequency 1e+6 Hz
3.6

@Frequency 1e+6 Hz
ASTM D150
4.0

@Frequency 60 Hz
4.0

@Frequency 60 Hz
ASTM D150
Dielectric Strength 11.8 - 15.7 kV/mm
300 - 400 kV/in
ASTM D149
Dissipation Factor 0.010

@Frequency 60 Hz
0.010

@Frequency 60 Hz
ASTM D150
Users viewing this material also viewed the following: