Quadrant EPP Fluorosint® MT-01 Enhanced PTFE (ASTM Product Data Sheet)  (Unverified Data**)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Fluorosint® MT-01 Enhanced PTFE (ASTM Product Data Sheet)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 2.27 g/cc
2.27 g/cc
ASTM D792
Water Absorption 0.10 %
0.10 %
Immersion, 24hr; ASTM D570(2)
Deformation 0.20 %
0.20 %
2000 psi; 122°F (50°C)
Mechanical Properties Metric English Comments
Hardness, Rockwell R 74
74
ASTM D785
Tensile Strength 14.5 MPa
2100 psi
ASTM D638
Elongation at Break 40 %
40 %
ASTM D638
Tensile Modulus 2.25 GPa
326 ksi
ASTM D638
Flexural Strength 27.6 MPa
4000 psi
ASTM D790
Flexural Modulus 3.34 GPa
485 ksi
ASTM D790
Compressive Strength 23.4 MPa
3400 psi
10% Def.; ASTM D695
Compressive Modulus 1.72 GPa
250 ksi
ASTM D695
Shear Strength 17.9 MPa
2600 psi
ASTM D732
Coefficient of Friction, Dynamic 0.18
0.18
dry vs. steel; QTM55007
K (wear) Factor 403 x 10-8 mm³/N-M
200 x 10-10 in³-min/ft-lb-hr
QTM55010
Limiting Pressure Velocity 0.158 MPa-m/sec
4500 psi-ft/min
4:1 safety factor applied; QTM 55010
Thermal Properties Metric English Comments
CTE, linear 54.0 µm/m-°C

@Temperature -40.0 - 150 °C
30.0 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E831
Maximum Service Temperature, Air 316 °C
600 °F
Continuous
Deflection Temperature at 1.8 MPa (264 psi) 93.3 °C
200 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 3.17 mm
V-0

@Thickness 0.125 in
Electrical Properties Metric English Comments
Surface Resistivity per Square <= 1.0e+6 ohm
<= 1.0e+6 ohm
ANSI/ESD STM 11.11
Compliance Properties Metric English Comments
3A-Dairy No
No
Canada AG No
No
FDA No
No
NSF No
No
USDA No
No
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Acceptable
Acceptable
Acids, Weak Acceptable
Acceptable
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Acceptable
Alkalies, Weak Acceptable
Acceptable
Chlorinated Solvents Acceptable
Acceptable
Conductive / Static Dissipative No
No
Continuous Sunlight Acceptable
Acceptable
Hot Water / Steam Limited
Limited
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Acceptable
Acceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Acceptable
Acceptable
Descriptive Properties Value Comments
Machinability 5
1-10, 1=Easier to Machine