Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil 111 Mobilux EP

Category Fluid , Lubricant , Lithium Gellant
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil 111 Mobilux EP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mobilux EP 111 is an extra high performance grease primarily designed for lubrication of all designs of couplings. It is specifically formulated to resist centrifugal separation of the oil from the soap thickener at extremely high rotating speeds, ensuring effective lubrication and protection against wear even in heavily loaded misaligned gear couplings. Mobilux EP 111 is a lithium hydroxystearate grease formulated with an extremely heavy, viscous mineral base oil. Mobilux EP 111 also contains an oil soluble molybdenum additive, as well as a very effective corrosion inhibitor. It is an NLGI 1 Grade grease. In addition to being used in a wide range of coupling designs, Mobilux EP 111 can also be used in low-speed open gearing and plain bearings. This grease has shown excellent performance and protection in a wide variety of coupling applications covering a broad range of industries. Based on its longstanding performance capabilities, this grease has become the product of choice for many users.Mobilux EP 111 is recommended for all types of heavily loaded lubricated couplings. Mobilux EP 111 has a recommended operating temperature range of -10 to 120º C. Mobilux EP 111 has performed very well in the following applications: Gear and grid couplings; Spring and slipper joint couplings; Spindle (gear) and chain couplings; Low speed open gears and plain bearings
Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 45 cSt
45 cSt
ASTM D445
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 315 kg
695 lb (mass)
ASTM D2596
Four Ball Wear 0.400 mm
0.0157 in
ASTM D2266
Penetration 325
325
Worked, 25°C; ASTM D217
Timken Test 22700 g
50.0 lb
Thermal Properties Metric English Comments
Dropping Point 180 °C
356 °F
ASTM D2265
Descriptive Properties Value Comments
Color black
Corrosion Prevention, ASTM D1743 pass
Soap/Thickener Type lithium