Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 2.00 - 20.0 kJ/m² | 0.952 - 9.52 ft-lb/in² | Average value: 8.39 kJ/m² Grade Count:45 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Notched (ISO) | 2.00 - 20.0 kJ/m² | 0.952 - 9.52 ft-lb/in² | Average value: 13.8 kJ/m² Grade Count:12 |
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and .. |
|||
Izod Impact, Notched (ISO) | 8.00 - 20.0 kJ/m² @Temperature -40.0 - -40.0 °C |
3.81 - 9.52 ft-lb/in² @Temperature -40.0 - -40.0 °F |
Average value: 11.5 kJ/m² Grade Count:4 |
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m.. |
|||
Izod Impact, Notched (ISO) | 8.00 - 20.0 kJ/m² @Temperature -30.0 - -30.0 °C |
3.81 - 9.52 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 12.6 kJ/m² Grade Count:4 |
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Izod Impact, Notched (ISO) | 20.0 - 20.0 kJ/m² @Temperature -40.0 - -40.0 °C |
9.52 - 9.52 ft-lb/in² @Temperature -40.0 - -40.0 °F |
Average value: 20.0 kJ/m² Grade Count:1 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |
|||
Izod Impact, Notched (ISO) | 11.0 - 20.0 kJ/m² @Temperature -40.0 - -20.0 °C |
5.23 - 9.52 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 14.6 kJ/m² Grade Count:17 |
Overview of materials for Nylon 6, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E.. |
|||
Izod Impact, Notched (ISO) | 3.00 - 20.0 kJ/m² | 1.43 - 9.52 ft-lb/in² | Average value: 8.40 kJ/m² Grade Count:37 |
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma.. |
|||
Izod Impact, Notched (ISO) | 9.70 - 20.0 kJ/m² | 4.62 - 9.52 ft-lb/in² | Average value: 15.6 kJ/m² Grade Count:7 |
Overview of materials for Nylon 610, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap.. |
|||
Izod Impact, Notched (ISO) | 15.0 - 20.0 kJ/m² | 7.14 - 9.52 ft-lb/in² | ISO 180 |
Tisan TISAKRIL® UNR ABS TISAKRIL has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include: High surface luminosityEasy processabilityDimens.. |
|||
Izod Impact, Notched (ISO) | 10.0 - 20.0 kJ/m² | 4.76 - 9.52 ft-lb/in² | Average value: 16.6 kJ/m² Grade Count:7 |
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max.. |
|||
Izod Impact, Notched (ISO) | 3.00 - 20.0 kJ/m² @Temperature -40.0 - -20.0 °C |
1.43 - 9.52 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 10.0 kJ/m² Grade Count:19 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |
|||
Izod Impact, Notched (ISO) | 5.00 - 20.0 kJ/m² | 2.38 - 9.52 ft-lb/in² | Average value: 9.75 kJ/m² Grade Count:4 |
Overview of materials for Polypropylene with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in.. |