Material Notes:
ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can originate from the interstices between the carbon black particle due to their complex arrangement and from the porosity.PROPERTIES: Very High StructureVery High Surface AreaHigh purityPERFORMANCE Electrical conductivity boosterUHF curing boosterFINAL APPLICATIONS: Power cable accessories, rollers, roller covering, microwave heating of thick rubber parts, shoe soles, heat shrinkable tubesInformation provided by TIMCAL
Physical Properties Metric English Comments
Density 0.135 g/cc
0.00488 lb/in³
Pour Density; ASTM D1513
Volatiles <= 0.30 %
<= 0.30 %
Weight loss during heating between 105 and 950°C; Internal Method 02
Oil Absorption 320 %
320 %
OAN (Oil Absorption Number) ml/100g; ASTM D2414
Particle Size 45 µm
45 µm
10 ppm sieve residue; ASTM D1514
pH 8.0 - 11
8.0 - 11
ASTM D1512
Specific Surface Area 770 m²/g
770 m²/g
BET Nitrogen Surface Area; ASTM D3037
Ash 0.030 %
0.030 %
ASTM D1506
Mechanical Properties Metric English Comments
Tensile Strength 64.8 MPa
9400 psi
Volume Resistivity 3 [log{ohm-cm)]
64.8 MPa
9400 psi
Volume Resistivity 10.3 [log{ohm-cm)]
65.8 MPa
9540 psi
Volume Resistivity 2.3 [log{ohm-cm)]
67.0 MPa
9720 psi
Volume Resistivity 2 [log{ohm-cm)]
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
Volume Resistivity 2 [log{ohm-cm)]
6.00 kJ/m²
2.86 ft-lb/in²
Volume Resistivity 3 [log{ohm-cm)]
7.00 kJ/m²
3.33 ft-lb/in²
Volume Resistivity 4.5 [log{ohm-cm)]
7.50 kJ/m²
3.57 ft-lb/in²
Volume Resistivity 10.5 [log{ohm-cm)]
Component Elements Properties Metric English Comments
Sulfur, S 0.020 %
0.020 %
ASTM D1619
Electrical Properties Metric English Comments
Volume Resistivity 6.0 ohm-cm
6.0 ohm-cm
6% Carbon Black in HDPE
10 ohm-cm
10 ohm-cm
15% Carbon Black in HDPE
100 ohm-cm
100 ohm-cm
10% Carbon Black in HDPE
1000 ohm-cm
1000 ohm-cm
8% Carbon Black in HDPE
Processing Properties Metric English Comments
Moisture Content <= 1.0 %
<= 1.0 %
as packed; ASTM D1509
Descriptive Properties Value Comments
Aspect Fine black granules
COAN (Crushed OAN) ml/100g 270
ASTM D3493
Toluene Extract, Max, % 0.1
ASTM D4527
Users viewing this material also viewed the following: