Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 4.20 J/cm² @Temperature 23.0 °C |
20.0 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PH 69 GF 20 T 10 PP, 20% glass fibre FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass fibre and 10 % Talc, contains themodifier of mechanical properties.Increased strength in comparison with .. |
|||
Charpy Impact Unnotched | 4.20 J/cm² @Temperature -20.0 °C |
20.0 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 GF 30 FRA 5 PA6, 30% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fibre, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°C,.. |
|||
Charpy Impact Unnotched | 4.20 J/cm² @Temperature -20.0 °C |
20.0 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 66 GF 13 TS PA66, 13% glass fibre FeaturesChemically reinforced with 13% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. W.. |
|||
Charpy Impact Unnotched | 4.20 J/cm² @Temperature 23.0 °C |
20.0 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVASTER® B2 GF 10 PBT, 10% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 10% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Charpy Impact Unnotched | 4.20 J/cm² @Temperature 23.0 °C |
20.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB SCANAMID 66.6 C12^F30 Nylon 66/6, Glass Fiber, Reinforced Information provided by Polykemi AB |
|||
Charpy Impact Unnotched | 4.20 J/cm² @Temperature -30.0 °C |
20.0 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® A ERV1906LK (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact Unnotched | 4.20 J/cm² @Temperature -20.0 °C |
20.0 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 GF 10 GB 20 PA6, 10% glass fibre, 20% glass beads FeaturesPA 6 for injection moulding, chemically strengthened with 10% glass fibre and 20% glass beads. Application: impacted mouldings and mouldings with high strength applied in automotive, electri.. |
|||
Charpy Impact Unnotched | 4.20 J/cm² @Temperature 23.0 °C |
20.0 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 6 T 30 TS PA6, 30% mineral filling FeaturesDecreased shrinkage against the BT types, increased heat application. Increased modulus in tension - strength of the material. PA matrix reduction. PA for injection moulding with the content.. |
|||
Charpy Impact Unnotched | 4.20 J/cm² @Temperature -30.0 °C |
20.0 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Ultem ATX202R PEI+PCE 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Charpy Impact Unnotched | 4.20 J/cm² @Temperature -30.0 °C |
20.0 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Charpy Impact Unnotched | 4.20 J/cm² @Temperature -30.0 °C |
20.0 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Charpy Impact Unnotched | 4.20 J/cm² @Temperature -30.0 °C |
20.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Sax Polymers SAXLAC 420HI Acrylonitrile Butadiene Styrene Saxalac 420HI is a flame retardant, very high flow ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provided.. |
|||
Charpy Impact Unnotched | 4.20 J/cm² @Temperature -20.0 °C |
20.0 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Borealis GB205U Polypropylene Compound, Glass Fiber Reinforced GB205U is a 20% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Thi.. |
|||
Charpy Impact Unnotched | 4.20 J/cm² @Temperature -20.0 °C |
20.0 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Borealis GD310U Polypropylene Compound, Glass Fiber Reinforced GD310U is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also at elevated temperatures. .. |
|||
Charpy Impact Unnotched | 4.20 J/cm² @Temperature 23.0 °C |
20.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1fU |
Borealis Nepol™ GB601HP Polypropylene, 30% Long Glass Fiber Reinforced w/HK060AE Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat.. |
|||
Charpy Impact Unnotched | 4.20 J/cm² @Temperature 23.0 °C |
20.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R513H Black Nylon 66, 13% Glass Reinforced, Conditioned Vydyne® R513H Black is general-purpose, 13% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is an injection-molding grade that is lubricated for machine feed, flow, and m.. |
|||
Charpy Impact Unnotched | 4.20 J/cm² @Temperature 23.0 °C |
20.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R513H Nylon 66, 13% Glass Filled, Conditioned (2.5% Moisture) Vydyne® R513H is general-purpose, 13% glass-reinforced, heat stabilized PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow, and mold .. |
|||
Charpy Impact Unnotched | 4.20 J/cm² @Temperature -20.0 °C |
20.0 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVASTER® B GB 40 PBT reinforced with glass beads PBT for injection molding, reinforced with 40% glass beads. Characterized by very good properties also at low temperature. Melt is characterized by very good rheology, which enables manufacturing of.. |
|||
Charpy Impact Unnotched | 4.20 J/cm² @Temperature -30.0 °C |
20.0 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® A CF350 (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact Unnotched | 4.20 J/cm² @Temperature 23.0 °C |
20.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Borealis MD231U Polypropylene Compound, Mineral Filled MD231U is a 20 % mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and a medium melt flow rate. Applications: Air duc.. |
|||
Charpy Impact Unnotched | 4.20 J/cm² @Temperature 23.0 °C |
20.0 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G45BL BK337 is a 45% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont .. |
|||
Charpy Impact Unnotched | 4.20 J/cm² @Temperature 23.0 °C |
20.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Sax Polymers SAXALEN PPC344G25 Polypropylene Copolymer, 25% Glass Filled SAXALEN PPC344G25 is a 25% glass filled Polypropylene - Copolymer intended for injection molding.Information provided by SAX Polymers |
|||
Charpy Impact Unnotched | 4.20 J/cm² @Temperature 23.0 °C |
20.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Sax Polymers SAXALEN PPH303G20 Polypropylene Homopolymer, 20% Glass Filled SAXALEN PPH303G20 is a 20% glass filled Polypropylene - Homopolymer injection molding grade with good stiffness.Information provided by SAX Polymers |