Radici Radilon® A ERV1906LK (cond.) Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Radici Group Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radilon® A ERV1906LK (cond.) Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information provided by Radici group.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 75.0 MPa
10900 psi
Elongation at Break 17 %
17 %
Nominal
Elongation at Yield 8.0 %
8.0 %
Tensile Modulus 4.20 GPa
609 ksi
Charpy Impact Unnotched 4.20 J/cm²

@Temperature -30.0 °C
20.0 ft-lb/in²

@Temperature -22.0 °F
10.0 J/cm²

@Temperature 23.0 °C
47.6 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.500 J/cm²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
1.50 J/cm²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Comparative Tracking Index 550 V
550 V