Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Iran Petrochemical (PCC) EX 3 - 80 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Pipe Grade
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) EX 3 - 80 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EX3-80 is a high density polyethylene with 1-Butene as co monomer. It is natural, good ESCR, good impact strength, tough and rigid pipe resin. Applications: pipe extrusion PE 80 class, industrial and pressure pipe , gas pipe, drinking water pipe, relining , fittings.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.945 g/cc
0.0341 lb/in³
ISO 1183
Environmental Stress Crack Resistance 50 hour

@Pressure 4.00 MPa
50 hour

@Pressure 580 psi
ISO CD 16770
Melt Flow 0.45 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.45 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
12 g/10 min

@Load 21.6 kg,
Temperature 190 °C
12 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ISO 868
Tensile Stress 35.0 MPa
5080 psi
at Break; ISO 527
Tensile Strength, Yield 22.0 MPa
3190 psi
ISO 527
Elongation at Break >= 850 %
>= 850 %
ISO 527
Elongation at Yield 8.0 %
8.0 %
ISO 527
Tensile Modulus 0.850 GPa
123 ksi
ISO 527
Charpy Impact, Notched 2.30 J/cm²
10.9 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Softening Point 67.0 °C
153 °F
ISO 306
Brittleness Temperature >= -80.0 °C
>= -112 °F
ASTM D746-72
Processing Properties Metric English Comments
Melt Temperature 190 - 220 °C
374 - 428 °F
Descriptive Properties Value Comments
Flexural Creep Modulus (MPa) 950
4 point, 1 min; DIN 19537-2