Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Iran Petrochemical (PCC) EX 5 HM 9450 F High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Film Grade
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) EX 5 HM 9450 F High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EX5 is a high density polyethylene with 1-Butene as co monomer.Applications: film extrusion, counter bag, carrier bag, wrapping filmsInformation provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.949 g/cc
0.0343 lb/in³
ISO 1183
Melt Flow 0.28 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.28 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
8.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
8.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ISO 868
Tensile Stress 35.0 MPa
5080 psi
at Break; ISO 527
Tensile Strength, Yield 24.0 MPa
3480 psi
ISO 527
Film Elongation at Break, MD <= 400 %
<= 400 %
ISO 527
Film Elongation at Break, TD <= 450 %
<= 450 %
ISO 527
Elmendorf Tear Strength MD 20.4 g
20.4 g
ISO 6383-2
Elmendorf Tear Strength TD 45.9 g
45.9 g
ISO 6383-2
Dart Drop Test 220 g
0.485 lb
ASTM D1709
Film Tensile Strength at Break, MD <= 45.0 MPa
<= 6530 psi
ISO 527
Film Tensile Strength at Break, TD <= 40.0 MPa
<= 5800 psi
ISO 527
Thermal Properties Metric English Comments
Softening Point 75.0 °C
167 °F
ISO 306
Brittleness Temperature >= -80.0 °C
>= -112 °F
ASTM D746-72
Processing Properties Metric English Comments
Melt Temperature 200 - 230 °C
392 - 446 °F