Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 64.0 - 66.0 MPa | 9280 - 9570 psi | DIN 53455 |
Zell-Metall Engineering Plastics Zellamid 1100 OIL Zellamid® 1100 OIL: A new type of cast nylon produced by addition of a special oil to the polymer structure. By laboratory test it was proven that this second generation oil filled product reduces .. |