Polymer Property : Tensile Strength at Break = 66.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 64.0 - 66.0 MPa
9280 - 9570 psi
DIN 53455
Zell-Metall Engineering Plastics Zellamid 1100 OIL
Zellamid® 1100 OIL: A new type of cast nylon produced by addition of a special oil to the polymer structure. By laboratory test it was proven that this second generation oil filled product reduces ..