Polymer Property : Tensile Strength at Break = 29200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 201 MPa
29200 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP LCL36 PEEK (Europe-Africa-Middle East)
LNP* LUBRICOMP* LCL36 is a compound based on Polyetheretherketone containing Carbon Fiber , PTFE. Added features of this material include Electrically Conductive, Internally Lubricated.
Tensile Strength at Break 201 MPa
29200 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP QCL34 PA6.10
LNP* LUBRICOMP* QCL34 is a compound based on Nylon 6/10 resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive.
Tensile Strength at Break 201 MPa
29200 psi
ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66
LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear Resistant.
Tensile Strength at Break 201 MPa
29200 psi
ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66 (Asia Pacific)
LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing Silicone, PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.
Tensile Strength at Break 201 MPa
29200 psi
ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66 (Europe-Africa-Middle East)
LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing Carbon Fiber, Silicone, PTFE. Added features of this material include: Electrically Conductive.
Tensile Strength at Break 201 MPa
29200 psi
ASTM D 638
SABIC Innovative Plastics LNP Stat-kon EE006EM PEI
LNP* Stat-kon* EE006EM is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding.This data was supplied by ..
Tensile Strength at Break 201 MPa
29200 psi
ASTM D 638
SABIC Innovative Plastics LNP Stat-kon EE006EM PEI (Asia Pacific)
LNP* Stat-kon* EE006EM is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding.This data was supplied by ..
Tensile Strength at Break 201 MPa
29200 psi
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP IC006 PA 6/12
LNP* THERMOCOMP* IC006 is a compound based on Nylon 6/12 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
Tensile Strength at Break 201 MPa
29200 psi
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP IC006 PA 6/12 (Asia Pacific)
LNP* Thermocomp* IC006 is a compound based on Nylon 6/12 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Tensile Strength at Break 201 MPa
29200 psi
ISO 527
SABIC Innovative Plastics LNP THERMOCOMP PF009 PA 6
LNP THERMOCOMP* PF009 is a compound based on Nylon 6 resin containing 45% Glass Fiber.
Tensile Strength at Break 201 MPa
29200 psi
ASTM D 638
SABIC Innovative Plastics LNP Stat-kon RE003 PA 66
LNP STAT-KON* RE003 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americ..
Tensile Strength at Break 201 MPa
29200 psi
ISO 527
SABIC Innovative Plastics LNP THERMOCOMP PF009 PA 6 (Asia Pacific)
LNP THERMOCOMP* PF009 is a compound based on Nylon 6 resin containing Glass Fiber.