Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 2.90 MPa | 420 psi | |
Shin-Etsu Silicones KE-347TUV Silicone, RTV Coating Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Tensile Strength at Break | 2.90 MPa | 420 psi | ASTM D412 |
Teknor Apex Uniprene® 35A Polyvinyl Chloride, Flexible Features: High Elastic RecoveryInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 2.90 MPa | 420 psi | ASTM D638 |
ExxonMobil Escorene® UL 7510 Adhesive Application Resin Escorene Ultra UL 7510 is a very high flow, 18.7% vinyl acetate copolymer that has very good compatibility with hydrocarbon tackifiers and most waxes. It is suitable for making hot melt adhesives, s.. |
|||
Tensile Strength at Break | 2.90 MPa | 420 psi | ASTM D638 |
ExxonMobil Escorene™ UL 7740 Ethylene Vinyl Acetate Copolymer Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: NoThermal Stabilizer: Yes Applications:Adhesives and SealantsIndustrial SealantsHot Melt AdhesivesWax Blends.. |
|||
Tensile Strength at Break | 2.90 MPa | 420 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 111-35 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Tensile Strength at Break | 2.90 MPa | 421 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 8211-35 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Tensile Strength at Break | 2.90 MPa @Time 436000 sec |
421 psi @Time 121 hour |
JRF-7 days |
3M AC-240 Class B-1/2 Aerospace Sealant 3M Aerospace Sealant AC-240 Class B is a two-part, polysulfide-based, long application life, quick cure product for use as a sealant for integral fuel tanks and fuselages. This tow-component, mangan.. |
|||
Tensile Strength at Break | 2.90 MPa @Time 436000 sec |
421 psi @Time 121 hour |
JRF-7 days |
3M AC-240 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-240 Class B is a two-part, polysulfide-based, long application life, quick cure product for use as a sealant for integral fuel tanks and fuselages. This tow-component, mangan.. |
|||
Tensile Strength at Break | 2.90 MPa | 420 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 191-55PA Thermoplastic Elastomer
(discontinued **) A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA-6 and blends thereof for applications where hard/soft .. |
|||
Tensile Strength at Break | 2.90 MPa @Time 436000 sec |
421 psi @Time 121 hour |
JRF-7 days |
3M AC-240 Class B-4 Aerospace Sealant 3M Aerospace Sealant AC-240 Class B is a two-part, polysulfide-based, long application life, quick cure product for use as a sealant for integral fuel tanks and fuselages. This tow-component, mangan.. |