Shin-Etsu Silicones KE-347TUV Silicone, RTV Coating

Category Polymer , Thermoset , Silicone
Manufacturer Shin-Etsu Silicones
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones KE-347TUV Silicone, RTV Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
Viscosity 100000 cP
100000 cP
Mechanical Properties Metric English Comments
Hardness, Shore A 30
30
Tensile Strength at Break 2.90 MPa
420 psi
Shear Strength 1.45 MPa
210 psi
Thermal Properties Metric English Comments
Thermal Conductivity 0.200 W/m-K
1.39 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Dielectric Strength 25.0 kV/mm
635 kV/in
Dissipation Factor 0.00010

@Frequency 60.0 Hz
0.00010

@Frequency 60.0 Hz
Processing Properties Metric English Comments
Cure Time 3.00 min
0.0500 hour
Tack Free Time
4320 min

@Temperature 23.0 °C
72.0 hour

@Temperature 73.4 °F
50% RH
Descriptive Properties Value Comments
Colors Translucent