Features: High Elastic RecoveryInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 35
35
5 seconds; ASTM D2240
Tensile Strength at Break 2.90 MPa
420 psi
ASTM D412
Elongation at Break 350 %
350 %
ASTM D412
100% Modulus 0.000827 GPa
0.120 ksi
ASTM D412
Tear Strength 11.0 kN/m
62.8 pli
Die C; ASTM D624
Compression Set 13 %

@Temperature -5.00 °C,
Time 79200 sec
13 %

@Temperature 23.0 °F,
Time 22.0 hour
Method B; ASTM D395
22 %

@Temperature 21.1 °C,
Time 79200 sec
22 %

@Temperature 70.0 °F,
Time 22.0 hour
Method B; ASTM D395
40 %

@Temperature 37.8 °C,
Time 79200 sec
40 %

@Temperature 100 °F,
Time 22.0 hour
Method B; ASTM D395