California Fine Wire Alloy 436L Precious Metal Alloy

Category Metal , Nonferrous Metal , Precious Metal
Manufacturer California Fine Wire
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF California Fine Wire Alloy 436L Precious Metal Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All values may vary dependent on specific design and usageProprietary compositionCapabilities: WireRibbonInsulatedInformation provided by California Fine Wire.
Physical Properties Metric English Comments
Density 22.2 g/cc
0.802 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 1290 MPa
187000 psi
Stress relieved
1380 MPa
200000 psi
Hard
Modulus of Elasticity 138 GPa
20000 ksi
Thermal Properties Metric English Comments
Melting Point 1870 °C
3398 °F
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000665 ohm-cm
0.0000665 ohm-cm
3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
Descriptive Properties Value Comments
Magnetic None
Temperature Coefficient of Resistance 0.00021 ohms/ohm-°C
0-100°C
Thermal EMF vs. Copper +0.007 mV