California Fine Wire Stablohm 812 Chromium, Aluminum, and Iron Resistance Wire

Category Metal , Electronic/Magnetic Alloy , Superalloy , Iron Base
Manufacturer California Fine Wire
Trade Name Stablohm
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF California Fine Wire Stablohm 812 Chromium, Aluminum, and Iron Resistance Wire.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Physical Properties Metric English Comments
Density 7.25 g/cc
0.262 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 793 MPa
115000 psi
Annealed
1210 MPa
175000 psi
Stress relieved
1380 MPa
200000 psi
Hard
Thermal Properties Metric English Comments
CTE, linear 11.8 µm/m-°C

@Temperature 20.0 °C
6.56 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.460 J/g-°C

@Temperature 20.0 °C
0.110 BTU/lb-°F

@Temperature 68.0 °F
Thermal Conductivity 19.0 W/m-K
132 BTU-in/hr-ft²-°F
Melting Point 1510 °C
2750 °F
Maximum Service Temperature, Air 1177 °C
2151 °F
Operating Temperature
Component Elements Properties Metric English Comments
Aluminum, Al 4.5 %
4.5 %
Chromium, Cr 21 %
21 %
Iron, Fe 74.5 %
74.5 %
as balance
Electrical Properties Metric English Comments
Electrical Resistivity 0.000135 ohm-cm
0.000135 ohm-cm
3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
Descriptive Properties Value Comments
Magnetic Strong
Temperature Coefficient of Resistance 0.00002 ohms/ohm-°C
0-100°C