Spartech Korad® SP-9071 FR/ABS Flame Retardant Sheet

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Sheet
Manufacturer Spartech
Trade Name Korad®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech Korad® SP-9071 FR/ABS Flame Retardant Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Flame Retardant SheetKorad is a registered trademark of Polymer Extruded Products, Inc..Information provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 99
99
ASTM D785
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Tensile Modulus 2.14 GPa
310 ksi
ASTM D638
Flexural Yield Strength 67.6 MPa
9800 psi
ASTM D790
Flexural Modulus 2.14 GPa
310 ksi
ASTM D790
Izod Impact, Unnotched 3.20 J/cm
6.00 ft-lb/in
ASTM D256
0.587 J/cm

@Temperature -40.0 °C
1.10 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Falling Dart Impact 31.2 J
23.0 ft-lb
73°F; ASTM D3029
13.6 J

@Temperature -40.0 °C
10.0 ft-lb

@Temperature -40.0 °F
ASTM D3029
Thermal Properties Metric English Comments
CTE, linear 101 µm/m-°C

@Temperature 20.0 °C
56.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 82.2 °C
180 °F
ASTM D648
Flammability, UL94 V-0
V-0
5V
Optical Properties Metric English Comments
Gloss 86 %
86 %
Gardner; ASTM D2523