Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plastics Group Polifil® RMC-20 20% Calcium Carbonate-Reinforced Polypropylene, High Impact

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
Manufacturer The Plastics Group of America
Trade Name Polifil®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastics Group Polifil® RMC-20 20% Calcium Carbonate-Reinforced Polypropylene, High Impact.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polifil® RMC series compounds are high impact polypropylenes reinforced with fine particle size calcium carbonate. In addition to the highest impact possible, they possess good stiffness, heat aging resistance, solvent resistance, surface quality, and good resistance to environmental stress-cracking.Applications: AutomotiveAppliancesElectrical componentsHousewaresVarious utility products Standard processing techniques are applicable. Information provided by The Plastics Group.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Filler Content 20 %
20 %
ASTM D2584
Linear Mold Shrinkage 0.013 cm/cm

@Thickness 1.59 mm
0.013 in/in

@Thickness 0.0625 in
ASTM D955
Melt Flow 8.0 - 12 g/10 min
8.0 - 12 g/10 min
230/2.16; May be specified; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 86
86
ASTM D785
Tensile Strength at Break 25.5 MPa
3700 psi
ASTM D638
Flexural Modulus 1.79 GPa
260 ksi
Tangent; ASTM D790
Izod Impact, Notched 0.801 J/cm
1.50 ft-lb/in
At 73°F; ASTM D256
Izod Impact, Unnotched 12.8 J/cm
24.0 ft-lb/in
At 73°F; ASTM D256
Gardner Impact 6.78 J
5.00 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
219 °F
ASTM D648