Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.600 - 7.21 J/cm | 1.12 - 13.5 ft-lb/in | Average value: 3.41 J/cm Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled". Each property range of values reported is m.. |
|||
Izod Impact, Unnotched | 6.80 - 7.20 J/cm @Temperature 23.0 °C |
12.7 - 13.5 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RKS 320 Rigid PVC, Antishock Extrusion Lead Free Various profiles, antishock |