Mechanical Properties Metric English Comments
Charpy Impact Unnotched 17.0 J/cm²

@Temperature -30.0 °C
80.9 ft-lb/in²

@Temperature -22.0 °F
Ineos ABS Lustran® E401
Very high surface resistance, high surface gloss.,Property data per ISO test methods.
Charpy Impact Unnotched 17.0 J/cm²

@Temperature 23.0 °C
80.9 ft-lb/in²

@Temperature 73.4 °F
80x10x4mm; ISO 179/1eU
SYNTHOS Forsan® 548 Acrylonitrile Butadiene Styrene (ABS)
Easy flow, glossy, impact resistant.Applications: General purposeVarious technical parts, household appliances, hobby and office equipment, etc.Synthos was formerly known as Kaucuk. All information ..
Charpy Impact Unnotched 17.0 J/cm²

@Temperature -30.0 °C
80.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
DuPont Performance Polymers Delrin® 100AL NC010 Acetal (POM)  (Unverified Data**)
Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 100AL NC010 an unreinforced high viscosity lubricated acetal homopolymer resin containing an advanced system of lub..
Charpy Impact Unnotched 17.0 J/cm²
80.9 ft-lb/in²
ISO 179/1eU
DuPont Performance Polymers Delrin® 500TL NC010 Acetal (POM)  (Unverified Data**)
Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500TL is a medium viscosity acetal homopolymer resin containing 1.5% Teflon PTFE Micropowder. It is desi..
Charpy Impact Unnotched 17.0 J/cm²

@Temperature -30.0 °C
80.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
DuPont Performance Polymers Delrin® FG100AL NC010 Acetal (POM)  (Unverified Data**)
Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin FG100AL is a high viscosity lubricated acetal homopolymer resin containing ..
Charpy Impact Unnotched 17.0 J/cm²
80.9 ft-lb/in²
ISO 179/1eU
DuPont Performance Polymers Delrin® FG500TL NC010 Acetal (POM)  (Unverified Data**)
Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact ApplicationsDelrin FG500TL medium viscosity acetal homopolymer resin containing 1.5%..
Charpy Impact Unnotched 17.0 J/cm²
80.9 ft-lb/in²
dry; ISO 179/1eU
EMS-Grivory Grivory® LKN-3H PA12-GB30
Product description: Grilamid LKN-3H is a 30% glass bead reinforced, heat stabilized polyamide 12 injection molding grade with the following property profile: Very low moisture absorptionExtremely g..
Charpy Impact Unnotched 17.0 J/cm²

@Temperature -30.0 °C
80.9 ft-lb/in²

@Temperature -22.0 °F
BASF Novolen® 2600 M Polypropylene, Injection Molding Grade
Injection molded partsData was collected by ISO methods and provided by BASF.
Charpy Impact Unnotched 17.0 J/cm²

@Temperature -30.0 °C
80.9 ft-lb/in²

@Temperature -22.0 °F
BASF Novolen® 2660 M Polypropylene
UV stabilized grade for injection molded parts.Data was collected by ISO methods and provided by BASF.
Charpy Impact Unnotched 17.0 J/cm²

@Temperature -30.0 °C
80.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179
BASF Ultraform S 2320 003 UNC Q600 POM
Ultraform S2320 003 UNC Q600 is an easy flowing and rapidly freezing injection molding POM grade. Contains a mold release agent.
Charpy Impact Unnotched 17.0 J/cm²
80.9 ft-lb/in²
ISO 179
BASF Ultraform S 1320 0021 UNC POM
Ultraform S1320 0021 UNC is an easy flowing, rapidly freezing injection molding POM grade with enhanced stiffness and heat distortion resistance. It is highly stabilized to resist aggressive fuels,..
Charpy Impact Unnotched 17.0 J/cm²

@Temperature -30.0 °C
80.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179
BASF Ultraform S 1320 0021 UNC POM
Ultraform S1320 0021 UNC is an easy flowing, rapidly freezing injection molding POM grade with enhanced stiffness and heat distortion resistance. It is highly stabilized to resist aggressive fuels,..
Charpy Impact Unnotched 17.0 J/cm² - NB
80.9 ft-lb/in² - NB
Average value: 17.0 J/cm² Grade Count:3
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum..
Charpy Impact Unnotched 17.0 J/cm²
80.9 ft-lb/in²
Polimeri Europa SINKRAL L320/G ABS, Platable Grade  (discontinued **)
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-25-16-20 Injection moulding grade, tailored for electroplating. It is a high flow grade with a good impact ..
Charpy Impact Unnotched 17.0 J/cm²
80.9 ft-lb/in²
Polimeri Europa SINKRAL L320 ABS  (discontinued **)
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-25-16-25 General purpose, high flow injection moulding grade having good impact resistance coupled with an ..